LOCTITE 425

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 425 LOCTITE 425

Main features

  • Fast Plated-Fastener Fixturing
  • Low-Strength Serviceable Retention
  • Pre- or Post-Applied Locking

Product Description

LOCTITE 425 is a dark-blue, low-viscosity, one-part cyanoacrylate adhesive for low-strength threadlocking and retaining on metal and plastic fasteners. It can be applied before or after assembly and cures with atmospheric moisture. On plated metal and plastic fasteners, fixture is achieved in less than two minutes, while full strength develops within 24 hours. The low-strength cured joint supports adjustment or disassembly rather than permanent locking. It is suited to tamperproofing screw heads and potentiometers and to serviceable fastener retention within the -54 to 85 deg C operating range.

Key features

  • Pre- or post-applied locking: The low-viscosity liquid can be placed before assembly or wicked onto assembled fasteners.
  • Fast plated-fastener fixture: Plated metal and plastic fasteners fixture in less than two minutes under documented conditions.
  • Low-strength serviceability: The cured adhesive provides low-strength retention for adjustment, tamperproofing, or later disassembly.

Applications / Suitable for

  • Low-strength locking of metal and plastic fasteners
  • Tamperproofing screw heads and potentiometers
  • Preassembled or post-applied retaining applications
Product Family

LOCTITE 425

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate / Aliphatic ester
Color
Dark blue liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
165 °C
Linear thermal expansion
100×10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
40 to 80 mPa.s
Electrical Properties
Dielectric Strength
19.7 kV/mm
Surface Resistivity
>1×10^15 Ohms Ohms/sq
Volume Resistivity
>1×10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceDark blue liquid-As supplied
Chemical typeEthyl cyanoacrylate / aliphatic ester-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity40 to 80mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time<2minPlated metal and plastic fasteners
Full-strength development24hNormal humidity-cure conditions
Operating temperature range-54 to 85deg CTypical application range
Dielectric breakdown strength19.7kV/mmIEC 60243-1
Volume resistivity>1 x 10^15ohm cmIEC 60093
Torque strength, 4-40 fastener0.12 / 0.14N mBreakaway / prevailing; zinc-plated, untorqued, cured 24 h at 22 deg C
Torque strength, 10-32 fastener0.36 / 0.23N mBreakaway / prevailing; zinc-plated, untorqued, cured 24 h at 22 deg C