LOCTITE 415

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 415

Main features

  • High-Viscosity Cyanoacrylate Adhesive
  • Documented MIL-A-46050C/A-A-3097 Qualification
  • Chemical and Environmental Resistance

Product Description

LOCTITE® 415™ is a one-component, high-viscosity methyl cyanoacrylate adhesive formulated for general-purpose instant bonding of metals, plastics and elastomers. It is particularly well suited for metal bonding applications and delivers rapid fixture speeds through moisture-activated curing. The adhesive provides strong structural performance, excellent environmental resistance, and reliable bonding on a wide range of substrates. LOCTITE 415 complies with Military Specification Mil-A-46050C and Commercial Item Description A-A-3097, making it suitable for demanding industrial and maintenance applications.

  • High-viscosity methyl cyanoacrylate adhesive.
  • Excellent bonding performance on metal substrates.
  • One-component formulation requiring no mixing.
  • Fast humidity-activated room-temperature cure.
  • Bonds metals, rubbers and plastics.
  • Qualified to Mil-A-46050C and A-A-3097 specifications.
  • Strong chemical and environmental resistance after cure.

Recommended Applications

  • Metal component assembly and bonding.
  • Rubber and plastic bonding applications.
  • Industrial manufacturing and maintenance repair.
  • General-purpose instant adhesive applications.
  • High-strength precision assemblies.
Product Family

LOCTITE 415

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear colorless slightly hazy to light yellow liquid
Specific Gravity
1.1
Physical Properties
Viscosity
1,100 - 1,600 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Methyl cyanoacrylate adhesive
Chemical Type Methyl Cyanoacrylate — General-purpose instant adhesive
Appearance Clear Colorless to Light Yellow Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.10 — 25°C
Viscosity (Cone & Plate) 900 - 1,500 mPa·s (cP) PHYSICA MK22 @ 100 s⁻¹, 25°C
Brookfield Viscosity 1,100 - 1,600 mPa·s (cP) LVF, Spindle 2, 12 rpm
Vapor Pressure <1 hPa Typical value
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/m·K ISO 8302
Volume Resistivity 2 × 10¹⁵ to 10 × 10¹⁵ Ω·cm IEC 60093
Surface Resistivity 10 × 10¹⁵ to 80 × 10¹⁵ Ω IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Lap Shear Strength (Steel) 20 - 30 N/mm² ISO 4587, Grit Blasted Steel
Lap Shear Strength (Aluminum) 15 - 22 N/mm² ISO 4587, Grit Blasted Aluminum
Tensile Strength (Steel) 12 - 25 N/mm² ISO 6922
Tensile Strength (Buna‑N) ≥6.0 N/mm² ISO 6922, 30 s Cure @ 22°C
T-Peel Strength (Steel) <0.5 N/mm ISO 11339