LOCTITE 414

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 414

Main features

  • Low-Viscosity General Bonding
  • Fast Rubber and Plastic Fixturing
  • Strong Thin-Gap Metal Bonds

Product Description

LOCTITE 414 is a one-part, low-viscosity ethyl cyanoacrylate instant adhesive for general-purpose bonding of plastics, rubbers, and metals. The transparent, colorless-to-straw liquid requires no mixing and cures with atmospheric moisture. At 22 deg C and 50% relative humidity, fixture times are under 5 seconds on neoprene and nitrile rubber, 2 to 10 seconds on aluminum, ABS, and PVC, and 15 to 30 seconds on degreased steel. After 24 hours at 22 deg C, grit-blasted steel lap shear strength is 18 to 26 N/mm^2. The adhesive performs best in thin 0.05 mm bond gaps.

Key features

  • Low-Viscosity General Bonding: The liquid flows into thin, close-fitting joints on plastics, rubbers, and metals.
  • Fast Rubber and Plastic Fixture: Neoprene and nitrile fixture in under 5 seconds; ABS and PVC fixture in 2 to 10 seconds.
  • Strong Thin-Gap Metal Bonds: Grit-blasted steel lap shear strength reaches 18 to 26 N/mm^2 after 24 hours.

Applications / Suitable for

  • General-purpose plastic bonding
  • Rubber and elastomer bonding
  • Thin-gap metal assembly
Product Family

LOCTITE 414

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate
Color
Transparent, colorless to straw colored liquid
Component System
One component
Specific Gravity
1.05
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Linear thermal expansion
80×10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Tack-Free Time
25 seconds minutes
Viscosity
100 to 150 mPa.s
Electrical Properties
Dielectric Strength
25 kV/mm
Volume Resistivity
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
15 -30 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw-Uncured
Specific gravity1.05-25 deg C
Viscosity70 to 110mPa sCone and plate, shear rate 3,000 s^-1, 25 deg C
Viscosity100 to 150mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion80 x 10^-6K^-1ISO 11359-2; cured 24 hours at 22 deg C
Thermal conductivity0.1W/(m K)ISO 8302; same cure
Glass transition temperature120deg CASTM E 228; same cure
Dielectric breakdown strength25kV/mmIEC 60243-1; same cure
Lap shear strength18 to 26N/mm^2Grit-blasted steel; cured 24 hours at 22 deg C
Lap shear strength11 to 19N/mm^2Etched aluminum; cured 24 hours at 22 deg C