LOCTITE 411

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 411

Main features

  • High-Viscosity Cyanoacrylate Gel
  • Controlled Non-Sag Application
  • High Peel Strength

Product Description

LOCTITE® 411™ is a one-component, high-viscosity ethyl cyanoacrylate adhesive gel designed for gap-filling applications involving rubbers, plastics and metals. The adhesive combines excellent peel strength with enhanced heat resistance while maintaining the rapid curing characteristics typical of cyanoacrylates. Its gel consistency prevents migration after application, allowing precise placement on vertical and irregular surfaces. LOCTITE 411 cures rapidly in the presence of atmospheric moisture and develops strong bonds across a wide range of substrates, making it suitable for industrial assembly, repair and maintenance applications. 

Key Features & Benefits

  • High-viscosity gel formulation with gap-filling capability.
  • Excellent peel strength compared with standard instant adhesives.
  • Enhanced heat resistance for demanding environments.
  • One-component adhesive requiring no mixing.
  • Fast humidity-activated cure at room temperature.
  • Suitable for bonding rubbers, plastics and metals.
  • Controlled non-sag application on vertical surfaces.

Recommended Applications

  • Gap-filling bonding applications.
  • Rubber-to-metal and plastic-to-metal assemblies.
  • General industrial assembly and maintenance.
  • Applications requiring improved peel strength.
  • Elevated-temperature bonding environments.
Product Family

LOCTITE 411

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Water white to slightly cloudy gel
Specific Gravity
1.05
Physical Properties
Viscosity
4,000 - 8,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Ethyl cyanoacrylate gel adhesive
Chemical Type Ethyl Cyanoacrylate — High-strength instant adhesive
Appearance Water White to Slightly Cloudy Gel — Uncured
Components One Part — No mixing required
Specific Gravity 1.05 — 25°C
Brookfield Viscosity 4,000 - 8,000 mPa·s (cP) RVT, Spindle TC, 20 rpm, 25°C
Key Substrates Rubbers, Plastics and Metals — Typical bonding materials
Cure Type Humidity Cure — Atmospheric moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 120 °C ASTM E228
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/m·K ISO 8302
Volume Resistivity 10 × 10¹⁵ Ω·cm IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Lap Shear Strength (Steel, Grit Blasted) 18 - 26 N/mm² ISO 4587, 24 h @ 22°C
Lap Shear Strength (Aluminum, Etched) 11 - 19 N/mm² ISO 4587, 24 h @ 22°C
Lap Shear Strength (ABS) >6 N/mm² ISO 4587, 24 h @ 22°C
Tensile Strength (Steel) 12 - 25 N/mm² ISO 6922, 24 h @ 22°C
Tensile Strength (Buna‑N) ≥7.0 N/mm² ISO 6922, 30 s @ 22°C
Lap Shear Strength at 121°C ≥8.3 N/mm² After 24 h @ 22°C + 24 h @ 121°C