LOCTITE 408

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 408 LOCTITE 408

Main features

  • Low-Odor Low-Blooming Bonding
  • Very-Low-Viscosity Joint Wetting
  • Rapid Porous-Material Fixturing

Product Description

LOCTITE 408 is a one-part, very-low-viscosity alkoxyethyl cyanoacrylate instant adhesive for rapid bonding of metals, plastics, elastomers, and absorbent materials. The transparent liquid cures with atmospheric moisture and is formulated for low odor and low blooming where vapor control is difficult. Fixture times are under 5 seconds on aluminum, neoprene, nitrile rubber, ABS, phenolic, leather, and paper at 22 deg C and 50% relative humidity, while other substrates require longer. The adhesive also bonds porous materials such as wood, paper, leather, and fabric. Its low viscosity suits thin, close-fitting joints and rapid assembly.

Key features

  • Low-Odor Low-Blooming Cure: The formulation reduces odor and blooming where vapor control is difficult.
  • Very-Low-Viscosity Flow: A 4 to 10 mPa s viscosity suits thin, close-fitting bondlines.
  • Porous-Material Bonding: Applications include wood, paper, leather, and fabric as well as metals, plastics, and elastomers.

Applications / Suitable for

  • Rapid bonding of metals, plastics, and elastomers
  • Bonding wood, paper, leather, and fabric
  • Low-odor, low-blooming assembly
Product Family

LOCTITE 408

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Alkoxyethyl cyanoacrylate
Color
Transparent, colorless to straw colored liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Linear thermal expansion
80×10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Tack-Free Time
25 seconds minutes
Viscosity
4 to 10 mPa.s
Electrical Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Curing Conditions
Fixture Time
20 -30 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw-Uncured
Specific gravity1.1-25 deg C
Viscosity4 to 10mPa sCone and plate, shear rate 3,000 s^-1, 25 deg C
Viscosity4 to 10mPa sBrookfield LVF, spindle 1, 60 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Lap shear strength20.8N/mm^2ISO 4587; grit-blasted steel; cured 72 hours at 22 deg C
Lap shear strength17.3N/mm^2ISO 4587; etched aluminum; same cure
Lap shear strength9.7N/mm^2ISO 4587; ABS; same cure
Lap shear strength8.6N/mm^2ISO 4587; polycarbonate; same cure
Block shear strength22.9N/mm^2ISO 13445; polycarbonate; same cure
Tensile strength27.3N/mm^2ISO 6922; steel pin to steel pin; cured 24 hours at 22 deg C