LOCTITE 4014

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

LOCTITE 4014 LOCTITE 4014 LOCTITE 4014

Main features

  • Very-Low-Viscosity Precision Bonding
  • Fast Mixed-Material Fixturing
  • Heat-Conditioned Bond Strength

Product Description

LOCTITE 4014 is a one-part, very-low-viscosity cyanoacrylate instant adhesive for fast room-temperature bonding of plastics and metals. The transparent, colorless-to-slightly-yellow liquid requires no mixing and cures with atmospheric moisture. Depending on the substrate pair, fixture times range from 5 to 30 seconds for many stainless-steel, ABS, polycarbonate, polyurethane, and G-10 epoxy combinations, while PVC-to-PVC fixtures in 60 to 80 seconds. After 24 hours at 22 deg C, the cured adhesive reaches Shore hardness 65 and 28 N/mm^2 tensile strength. It is also intended for disposable medical-device assembly within the product-specific evaluation scope.

Key features

  • Very-Low-Viscosity Flow: A 1 to 5 mPa s viscosity suits thin, close-fitting plastic and metal joints.
  • Fast Mixed-Material Fixture: Many stainless-steel-to-plastic combinations fixture in 5 to 10 seconds.
  • Heat-Conditioned Strength: Grit-blasted steel lap shear remains at least 12 N/mm^2 after a 24-hour, 121 deg C heat condition.

Applications / Suitable for

  • Fast bonding of plastics and metals
  • Stainless-steel-to-plastic assembly
  • Disposable medical-device assembly
Product Family

LOCTITE 4014

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent, colorless to slightly yellow liquid
Component System
One component
Specific Gravity
1.1
Physical Properties
Viscosity
1 to 4 mPa.s
Mechanical Properties
Elongation
2 %
Curing Conditions
Fixture Time
60 to 80 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to slightly yellow-Uncured
Specific gravity1.1-25 deg C
Viscosity1 to 4mPa sCone and plate, shear rate 100 s^-1, 25 deg C
Viscosity1 to 5mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Shore hardness65-ISO 868; cured 24 hours at 22 deg C
Elongation2%ISO 527-2; same cure
Tensile strength28N/mm^2ISO 527-3; same cure
Lap shear strength>7.5N/mm^2PVC to PVC; cured 24 hours at 22 deg C
Lap shear strength>5.5N/mm^2Stainless steel to ABS; cured 24 hours at 22 deg C
Lap shear strength>=12N/mm^2Grit-blasted steel; cured 24 hours at 22 deg C, then 24 hours at 121 deg C; tested at 22 deg C