LOCTITE 4013

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 4013

Main features

  • Medium-Viscosity Cyanoacrylate Adhesive
  • ISO 10993 Biocompatibility
  • Disposable Medical-Device Assembly

Product Description

LOCTITE® 4013™ is a one-part, medium-viscosity ethyl cyanoacrylate adhesive formulated for rapid bonding of plastics and metals. Designed specifically for the assembly of disposable medical devices, the adhesive cures quickly at room temperature through exposure to ambient humidity and provides fast fixture times on a wide variety of substrates. LOCTITE 4013 has been evaluated using Henkel test protocols based on ISO 10993 biocompatibility standards, making it suitable for medical device manufacturing applications where dependable performance and rapid production throughput are required. The transparent adhesive delivers strong bonds, excellent handling characteristics and reliable mechanical performance after cure.

Key Features & Benefits

  • One-component cyanoacrylate adhesive requiring no mixing.
  • Fast room-temperature curing through ambient humidity.
  • Designed for plastics and metal bonding applications.
  • Medium viscosity supports controlled dispensing and gap filling.
  • Suitable for disposable medical device assembly.
  • Evaluated using ISO 10993 biocompatibility test protocols.
  • Excellent fixture speed and handling strength development.

Recommended Applications

  • Disposable medical device assembly.
  • Plastic-to-plastic bonding.
  • Plastic-to-metal bonding.
  • General-purpose industrial assembly requiring rapid cure.
  • Precision bonding of small components.
Product Family

LOCTITE 4013

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.1
Physical Properties
Viscosity
400 - 800 mPa.s
Mechanical Properties
Elongation
2 %

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Humidity curing adhesive
Appearance Transparent, Colorless to Slightly Yellow Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.1 — 25°C
Viscosity 400 - 800 mPa·s (cP) Brookfield LVF, Spindle 2, 30 rpm, 25°C
Key Substrates Plastics and Metals — Typical bonding applications
Cure Type Humidity Cure — Ambient moisture activation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Tensile Strength 28 N/mm² ISO 527-3, 24 h @ 22°C
Shore Hardness 65 Shore D ISO 868
Lap Shear Strength (Steel, Grit Blasted) ≥12 N/mm² 24 h cure @ 22°C
Lap Shear Strength (PVC to PVC) >5 N/mm² 24 h cure @ 22°C
Lap Shear Strength (ABS to ABS) >4 N/mm² 24 h cure @ 22°C
Lap Shear Strength (Polycarbonate to Polycarbonate) >7 N/mm² 24 h cure @ 22°C
Fixture Time (ABS to ABS) 5 - 10 seconds Typical room-temperature cure
Fixture Time (Polycarbonate to Polycarbonate) 10 seconds Typical room-temperature cure
Tensile Strength (Buna-N, 10 s Cure) ≥6.9 N/mm² ISO 6922