LOCTITE 3922

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 3922 LOCTITE 3922

Main features

  • Low-Viscosity Cannula Bonding
  • Fast UV/Visible-Light Fixturing
  • Sterilization-Tested Needle Assemblies

Product Description

LOCTITE AA 3922 is a one-component, low-viscosity UV/visible-light acrylic adhesive for rapid needle assembly and other precision medical-device bonding. The transparent-to-hazy liquid requires no mixing, fluoresces under UV light for presence inspection, and fixtures glass in 10 seconds or less under the specified 365 nm exposure. It bonds stainless steel cannulae into hubs, syringes, and lancets. Cannula-bonding results cover multiple hub polymers and sterilization methods. At the specified cure condition, the material has 135% elongation, Shore D 66, and 18 N/mm^2 tensile strength. Its flow and cure profile suit small bond areas and controlled cannula placement.

Key features

  • Low-Viscosity Cannula Bonding: A 150 to 450 mPa s viscosity supports controlled flow around small cannula-to-hub joints.
  • Fast Light Fixture: Glass fixture strength develops in 10 seconds or less at the listed 365 nm condition.
  • Sterilization-Tested Assemblies: Tested needle assemblies retained bond strength after listed gamma, EtO, and autoclave cycles.

Applications / Suitable for

  • Bonding stainless steel cannulae into hubs
  • Syringe and lancet needle assembly
  • Disposable medical-device assembly
Product Family

LOCTITE 3922

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent to hazy liquid
Chemistry Type
UV acrylic
Component System
One component
Specific Gravity
1.04
Thermal Properties
Glass Transition Temperature (Tg)
75 °C
Physical Properties
Tack-Free Time
>60 minutes
Viscosity
150 to 450 mPa.s
Chemical Properties
Water Absorption
7.2 %
Mechanical Properties
Elongation
135 %
Electrical Properties
Dielectric Strength
37 kV/mm
Volume Resistivity
1.06×10^14 Ohms⋅cm
Curing Conditions
Fixture Time
≤10 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent to hazy-Uncured
UV fluorescencePositive-Uncured material under UV light
Specific gravity1.04-25 deg C
Viscosity150 to 450mPa sCone and plate, shear rate 1,000 s^-1, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Glass transition temperature75deg CISO 11359-2; cured 30 seconds per side at 100 mW/cm^2 and 365 nm
Shore hardness66Durometer DISO 868; same cure
Elongation at break135%ISO 527-3; same cure
Tensile strength18N/mm^2ISO 527-3; same cure
Tensile modulus630N/mm^2ISO 527-3; same cure
Block shear strength23.5N/mm^2ISO 13445; polycarbonate to polycarbonate; same cure