LOCTITE 380

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 380

Main features

  • Rubber-Toughened Shock Resistance
  • Black Bondline Identification
  • Fast Multi-Substrate Fixturing

Product Description

LOCTITE 380 is a one-part, medium-viscosity ethyl cyanoacrylate instant adhesive for bonding metals, plastics, and rubbers. The black liquid cures with atmospheric moisture and is rubber toughened to increase flexibility, peel strength, and shock resistance. Fixture times vary by substrate, ranging from 10 to 30 seconds on aluminum and 60 to 120 seconds on degreased steel at 22 deg C and 50% relative humidity. After 24 hours at 22 deg C, grit-blasted steel lap shear strength is 26 N/mm^2. The adhesive performs best in thin bond gaps and is suited to assemblies requiring a black, impact-resistant instant bond.

Key features

  • Rubber-Toughened Bond: The cured adhesive provides increased flexibility, peel strength, and shock resistance.
  • Black Bondline: The black liquid provides a visible bondline for dark or opaque assemblies.
  • Substrate-Specific Fixture: Fixture times range from seconds to minutes depending on the bonded material.

Applications / Suitable for

  • Instant bonding of metals
  • Bonding plastics and rubbers
  • Black, shock-resistant close-fitting joints
Product Family

LOCTITE 380

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate
Color
Black liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Linear thermal expansion
80×10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Tack-Free Time
25 seconds minutes
Viscosity
100 to 800 mPa.s
Electrical Properties
Dielectric Strength
25 kV/mm
Volume Resistivity
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
60 -120 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceBlack liquid-Uncured
Specific gravity1.1-25 deg C
Viscosity100 to 800mPa sBrookfield RVT, spindle 3, 50 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion80 x 10^-6K^-1ISO 11359-2; cured 24 hours at 22 deg C
Thermal conductivity0.1W/(m K)ISO 8302; same cure
Glass transition temperature120deg CASTM E 228; same cure
Dielectric breakdown strength25kV/mmIEC 60243-1; same cure
Lap shear strength26N/mm^2ISO 4587; grit-blasted steel; cured 24 hours at 22 deg C
Tensile strength18.5N/mm^2ISO 6922; grit-blasted steel; cured 24 hours at 22 deg C