LOCTITE 363

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE 363

Main features

  • Low-Viscosity Shallow Potting
  • Rapid 365 nm UV Cure
  • Dielectric Electronic Encapsulation

Product Description

LOCTITE AA 363 is a one-component, low-viscosity urethane methacrylate material for UV-light shallow potting and thin-film encapsulation. The transparent yellow liquid requires no mixing and flows into electronic assemblies that need photocured protection. Typical cure is 20 to 30 seconds at 100 mW/cm^2 with a 365 nm medium-pressure mercury lamp, with a 25-second tack-free time at the same wavelength and intensity. After cure, the material reaches Shore D 50 and has a dielectric breakdown strength of 34 kV/mm. Its function is limited to shallow electronic potting and thin protective encapsulation layers.

Key features

  • Low-Viscosity Encapsulation: A 100 to 400 mPa s viscosity supports shallow potting and thin-film coverage.
  • Rapid UV Cure: Typical cure is 20 to 30 seconds at 100 mW/cm^2 and 365 nm.
  • Electrical Insulation: The cured material provides 34 kV/mm dielectric breakdown strength under the listed test method.

Applications / Suitable for

  • Shallow potting of electronic assemblies
  • Thin-film encapsulation of electronic assemblies
Product Family

LOCTITE 363

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Acrylated urethane
Color
Transparent yellow liquid
Component System
One component
Specific Gravity
1.1
Physical Properties
Tack-Free Time
25 seconds minutes
Viscosity
100 to 400 mPa.s
Electrical Properties
Dielectric Strength
34 kV/mm
Volume Resistivity
2×10^15 Ohms⋅cm
Physical Properties
Depth of Cure
15 mm
Curing Conditions
Fixture Time
5 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent yellow-Uncured
Specific gravity1.1-25 deg C
Viscosity100 to 400mPa sBrookfield RVT, spindle 1, 20 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Coefficient of thermal expansion100 x 10^-6K^-1ISO 11359-2; cured material
Thermal conductivity0.1W/(m K)ISO 8302; cured material
Shore hardness50Durometer DISO 868; cured material
UV depth of cure>=1.8mm100 mW/cm^2 at 365 nm for 20 seconds
Dielectric breakdown strength34kV/mmIEC 60243-1; cured material
Volume resistivity2 x 10^15ohm cmIEC 60093; cured material
Tensile strength3 to 12N/mm^2ISO 6922; steel pin to glass; cured 20 seconds at 100 mW/cm^2 and 365 nm

Leading Brands Trust in Our Products and Services