LOCTITE 3621

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3621

Main features

  • One component
  • Chipbonder
  • Very High dispense speed

Product Description

LOCTITE 3621 epoxy adhesive is a Chipbonder designed for the bonding of surface mounted devices to printed circuit boards prior to wave soldering. Particularly suited for applications where very high dispense speeds, high dot profile, high wet strength and good electrical characteristics are required. Particularly suited where dispense speeds greater than 35,000 dots/h are required. Dispense speed ranges from 25000 to 50000 dots per hour.

LOCTITE 3621 has been used successfully for small part bonding in lead free processes with water and alcohol based fluxes under conditions outlined in the Environmental Resistance section.

Cure schedule

  • 30 minutes @ 150°C 

Note: Sufficient time must be added to allow the bond location to reach the desired cure temperature. Curing profiles should be developed for each device. Bond strength achieved in practice will vary considerably depending on the SMD component type, adhesive dot size and the type, grade and degree of cure of the solder mask/resist.

Product Family

LOCTITE 3621

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.22
Thermal Properties
Glass Transition Temperature (Tg)
110 °C
Thermal Conductivity
0.3 W/m.K
Electrical Properties
Volume Resistivity
1300000000000000 Ohms⋅cm
Physical Properties
Viscosity
3,000 mPa.s