LOCTITE 3508NH

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3508NH

Main features

  • Reworkable
  • Reflow curable
  • Improves mechanical reliability

Product Description

This product was discontinued at the end of Q2 2022.  If you are looking for an alternative for this cornerbond material you can look into LOCTITE 3515. 

LOCTITE 3515 has a faster curing speed than 3508NH. LOCTITE 3515 was originally designed to cure together with SnPb solder reflow profile (~245 Celsius) and 3508NH was designed for Pb free SAC solder reflow profile (~260 Celsius). 

 

LOCTITE® 3508NH is designed to cure during Pb-free solder reflow while allowing self-alignment of IC components. It can be pre-applied to the board at the corners of the pad site using a standard SMA dispenser.

LOCTITE® 3508NH is a halogen free reworkable "Cornerbond" underfill that eliminates post reflow dispenses and cure steps while also improving mechanical reliability of handheld devices.

Cure Schedule

  • Pb-free solder reflow profile @ 245°C

With all curing systems, the time required for cure depends on the rate of heating. Conditions where a hot plate or a heat sink is used are optimum for fastest cure. Cure rates depend on the mass of material to be heated and intimate contact with the heat source. Use suggested cure conditions as general guidelines. Other cure conditions may yield satisfactory results.

Product Family

LOCTITE 3508NH

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.23
Thermal Properties
Glass Transition Temperature (Tg)
118 °C
Physical Properties
Viscosity
70,000 mPa.s

Additional Information

Visualization of the cornerbond process for stress relief

 

LOCTITE® 3508NH application in practice.

Leading Brands Trust in Our Products and Services