LOCTITE 3211

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 3211

Main features

  • UV/Visible-Light Cure Activation
  • Fast Adhesive Cure
  • Low-Viscosity Adhesive Application

Product Description

LOCTITE® AA 3211 LC is a one-component ultraviolet and visible light-curing acrylic adhesive formulated for rapid bonding of plastics, glass and metal substrates. Its clear, low-viscosity formulation enables fast curing under appropriate UV light sources while producing transparent, durable bonds. The adhesive is particularly suitable for applications requiring optical clarity, efficient processing and good adhesion across a broad range of materials. Once cured, LOCTITE AA 3211 provides a balance of strength, flexibility and environmental resistance, making it suitable for industrial, electronic and general assembly applications.

Key Features & Benefits

  • UV and visible light-curing acrylic adhesive
  • One-component system requiring no mixing.
  • Clear, transparent cured appearance.
  • Fast curing for high-throughput manufacturing processes.
  • Good adhesion to plastics, glass and metal substrates.
  • Low viscosity for easy dispensing and penetration into close-fitting assemblies.
  • Suitable for transparent bonding applications requiring optical clarity.

Recommended Applications

  • Plastic-to-plastic bonding assemblies.
  • Glass-to-plastic and glass-to-metal bonding.
  • Electronic and industrial component assembly.
  • Optically clear bonding applications.
  • Manufacturing environments utilizing UV curing equipment.
Product Family

LOCTITE 3211

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.48
Specific Gravity
1.13
Physical Properties
Viscosity
8,000 - 14,500 mPa.s
Mechanical Properties
Elongation
260 %

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — UV / Visible Light Cure
Chemical Type Acrylic Adhesive — Light-curing system
Appearance Clear Liquid — As supplied
Odor Mild — As supplied
Density 1.164 g/cm³ 20°C
Dynamic Viscosity 25 mPa·s Shear gradient 15 s⁻¹
Flash Point 86 °C Pensky-Martens Closed Cup
Initial Boiling Point >93 °C Typical property
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Cured Appearance Clear / Transparent — UV-cured adhesive
Adhesion Performance High — Glass, metals and plastics
UV Cure Mechanism Photopolymerization — Ultraviolet / visible light exposure
Volume Stability Excellent — Crosslinked cured network
Environmental Resistance Good — Industrial service conditions
Electrical Insulation Characteristics Good — Typical cured acrylic adhesive
Optical Clarity Excellent — Transparent bond lines