LOCTITE 3128 is a one part, heat curable epoxy designed to cure at low temperature and gives excellent adhesion on a wide range of materials in considerably short time. Typical applications include Memory cards, CCD/CMOS Assemblies and Lid/Cap attach for automotive optical sensors and 3d sensing modules.

LOCTITE 3128 can be successfully used as an Edgebond underfill, particularly suited where low curing temperatures are required for heat sensitive components. This low halogen, high viscosity, heat curable epoxy has a good adhesion to a variety of surfaces and a whopping 3 weeks of pot life.

LOCTITE 3128 has a fairly low CTE and warpage and as such has also been used on finger print sensor encapsulation with positive results. This is a camera/sensor market material so is not expected to pass very harsh reliability requirements.

Recommended cure schedule

  • 20 minutes @ 80°C bondline temperature
  • 60 minutes @ 60 °C bondline temperature

Note: Sufficient time must be added to allow the bond location to reach the desired cure temperature. Curing profiles should be developed for each device.

Product Family

LOCTITE 3128

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 52 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.6
Thermal Properties
Glass Transition Temperature (Tg)
45 °C
Mechanical Properties
Elongation
2.3 %
Physical Properties
Viscosity
27,000 mPa.s