LOCTITE 3104

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 3104

Main features

  • UV/Visible-Light Adhesive Cure
  • Direct PVC-to-Polycarbonate Bonding
  • Low-Viscosity Adhesive Application

Product Description

LOCTITE® AA 3104™ is a one-component UV and visible light-curing acrylic adhesive designed primarily for bonding rigid or flexible PVC to polycarbonate. The transparent liquid formulation cures rapidly upon exposure to ultraviolet or visible light, enabling high-speed manufacturing processes and efficient assembly operations. Its low-viscosity characteristics allow easy application in close-fitting assemblies, while the cured adhesive provides flexibility that enhances load-bearing and shock-absorbing performance. LOCTITE AA 3104 demonstrates excellent adhesion to a broad range of substrates including polycarbonate, PVC, glass, many plastics and most metals.

Key Features & Benefits

  • UV and visible light-curing adhesive for rapid production processing.
  • Specifically developed for bonding PVC to polycarbonate.
  • Transparent formulation for aesthetically clean bond lines.
  • Low-viscosity adhesive supports easy dispensing and wetting.
  • Flexible cured bond enhances shock absorption and load distribution.
  • One-component system requiring no mixing.
  • Excellent adhesion to plastics, glass and metal substrates.

Recommended Applications

  • Polycarbonate-to-PVC bonding.
  • Joining flexible PVC tubing to polycarbonate components.
  • Transparent plastic assembly applications.
  • Glass-to-plastic and plastic-to-metal bonding.
  • High-speed manufacturing processes utilizing UV curing systems.
Product Family

LOCTITE 3104

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.48
Specific Gravity
1.13
Physical Properties
Viscosity
90 - 210 mPa.s
Mechanical Properties
Elongation
50 %

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — UV / Visible Light Cure
Chemical Type Acrylated Urethane — One-component adhesive
Appearance Transparent Liquid — Uncured
Components One Component — No mixing required
Viscosity 90 - 210 mPa·s (cP) Brookfield RVT, 25°C
Specific Gravity 1.13 — 25°C
Refractive Index 1.48 — ASTM D542
Fixture Time <5 to 15 seconds Depending on light source and intensity
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Tensile Strength at Break 19 N/mm² ISO 527-3
Tensile Modulus 738 N/mm² ISO 527-3
Elongation at Break 50 % ISO 527-3
Shore Hardness 69 Shore D ISO 868
Refractive Index 1.51 — ASTM D542
Lap Shear Strength (Polycarbonate to PVC) 9.78 N/mm² Initial strength
Lap Shear Strength (Polycarbonate to Polycarbonate) 21.8 N/mm² Initial strength
Dielectric Breakdown Strength 34 kV/mm IEC 60243-1
Volume Resistivity 0.92 × 10¹⁵ Ω·cm IEC 60093