LOCTITE 277

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 277

Main features

  • M25 Bolt/Stud Threadlocking
  • High-Strength Thread Retention
  • Medium-Viscosity Threadlocking Application

Product Description

LOCTITE® 277 is a high-strength anaerobic threadlocking adhesive designed for the permanent locking and sealing of threaded fasteners. The one-component acrylic formulation cures when confined between closely fitting metal surfaces in the absence of air, preventing loosening and leakage caused by shock, vibration and dynamic loading. LOCTITE 277 is particularly suited for large bolts and studs (M25 and larger) where maximum holding power is required. The cured adhesive delivers excellent resistance to oils, fuels, chemicals and environmental exposure while maintaining reliable performance across a wide temperature range. Its fluorescent properties under UV light also support inspection and quality-control processes. High-strength threadlocker for permanent locking and sealing applications.

  • Prevents loosening caused by vibration, shock and dynamic loads.
  • Specifically designed for large bolts and studs (M25 and larger).
  • One-component anaerobic formulation requiring no mixing.
  • Fluorescent under UV light for inspection purposes
  • Excellent resistance to motor oil, fuel, brake fluid, water/glycol mixtures and chemicals.
  • Suitable for demanding industrial, maintenance and heavy-equipment applications.

Recommended Applications

  • Permanent locking of large threaded fasteners.
  • Heavy-duty industrial equipment and machinery.
  • Large bolts, studs and structural assemblies.
  • Equipment exposed to vibration and dynamic loading.
  • Applications requiring high resistance to chemicals and fluids.
Product Family

LOCTITE 277

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red liquid
Specific Gravity
1.12
Physical Properties
Viscosity
6,000 - 8,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component adhesive
Color Red — Liquid
Fluorescence Positive Under UV Light — Inspection aid
Specific Gravity 1.12 — 25°C
Brookfield Viscosity 6,000 - 8,000 mPa·s RVT, spindle 4, 20 rpm, 25°C
Strength Classification High — Threadlocking adhesive
Flash Point 165 °C Cleveland Open Cup
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 32 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Prevail Torque 32 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Breakloose Torque 38 N·m ISO 10964, pre-torqued to 5 N·m
Maximum Prevail Torque 40 N·m ISO 10964, pre-torqued to 5 N·m
Compressive Shear Strength ≥9 N/mm² ISO 10123, steel pins and collars
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Cold Temperature Capability -75 °C Tested minimum temperature
Chemical Resistance Excellent — Resists motor oil, gasoline, brake fluid, ethanol and industrial chemicals