LOCTITE 2701

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 2701

Main features

  • High-Strength Thread Retention
  • Low-Viscosity Threadlocking Application
  • Fluorescent Under UV Light

Product Description

LOCTITE® 2701 is a high-strength anaerobic threadlocking adhesive designed for the permanent locking and sealing of threaded metal fasteners. The one-component acrylic formulation cures in the absence of air between closely fitting metal surfaces, preventing loosening and leakage caused by shock and vibration. LOCTITE 2701 is particularly well suited for inactive metal substrates such as stainless steel and plated metals, and for applications requiring maximum resistance to hot oils. The low-viscosity adhesive penetrates threads efficiently while providing strong locking performance, excellent chemical resistance and long-term durability in demanding industrial environments.

Key Features & Benefits

  • High-strength threadlocker for permanent fastener locking and sealing.
  • Designed for inactive metals including stainless steel and plated surfaces.
  • Excellent resistance to hot oils and industrial fluids.
  • Prevents loosening caused by vibration, shock and dynamic loading.
  • Low-viscosity formulation promotes efficient thread penetration.
  • One-component anaerobic adhesive requiring no mixing.
  • Fluorescent under UV light for inspection and quality control.

Recommended Applications

  • Permanent locking of threaded fasteners.
  • Sealing threaded assemblies against leakage.
  • Fasteners subjected to shock and vibration.
  • Assemblies operating in hot-oil environments.
  • Industrial machinery, pumps, gearboxes and maintenance applications.
Product Family

LOCTITE 2701

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Green liquid
Specific Gravity
1.08
Physical Properties
Viscosity
500 - 900 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component
Color Green — Liquid
Strength Classification High — Threadlocking adhesive
Viscosity 500 - 900 mPa·s Brookfield RVT, 25°C
Specific Gravity 1.08 — 25°C
Density 1.10 g/ml 20°C
Flash Point 100 °C Closed cup
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 26 - 50 N·m ISO 10964, M10 black oxide steel nuts and bolts
Prevail Torque ≥15 N·m ISO 10964, M10 black oxide steel nuts and bolts
Breakloose Torque 30 - 60 N·m ISO 10964, pre-torqued to 5 N·m
Maximum Prevail Torque 36 - 60 N·m ISO 10964, pre-torqued to 5 N·m
Compressive Shear Strength 18 - 30 N/mm² ISO 10123, steel pins and collars
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Specific Heat 0.3 kJ/(kg·K) Typical cured value

Leading Brands Trust in Our Products and Services