LOCTITE 2620

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 2620 LOCTITE 2620

Main features

  • Elevated-Temperature Threadlocking Paste
  • Thixotropic Paste Placement
  • Medium-to-High Fastener Retention

Product Description

LOCTITE 2620 is a red, high-viscosity anaerobic threadlocker paste for locking and sealing metal fasteners in elevated-temperature assemblies. The one-component material requires no mixing and cures without air between close-fitting metal surfaces. Its thixotropic paste consistency supports controlled placement on threads, while the medium-to-high cured strength resists loosening and leakage under shock and vibration. High-temperature resistance is a primary selection factor for this grade. Torque performance applies to the specified steel and phosphate-and-oil fastener configurations under the defined cure conditions.

Key features

  • Extreme-temperature positioning: The formulation is intended for threaded assemblies requiring elevated-temperature resistance.
  • Thixotropic paste placement: High viscosity helps maintain coverage on threaded surfaces before assembly.
  • Medium-to-high retention: Cured joints resist loosening and leakage under shock and vibration.

Applications / Suitable for

  • Locking and sealing threaded metal fasteners
  • Shock- and vibration-exposed threaded assemblies
  • Elevated-temperature fastener applications
Product Family

LOCTITE 2620

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Paste
Chemistry Type
Dimethacrylate ester
Color
Red
Component System
1K
Specific Gravity
1.16
Physical Properties
Viscosity
20,000 to 70,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
AppearanceRed paste-Uncured
ComponentsOne-No mixing required
Cure mechanismAnaerobic-Secondary cure with activator when required
Specific gravity1.16-Typical at 25 deg C
Viscosity20,000 to 70,000mPa sCone and plate; 50 mm parallel plates; 0.5 mm gap; 50 s^-1; 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakloose torque11.4 to 34N mISO 10964; pretorqued 5 N m; degreased 3/8 x 16 grade 5 steel; cured 24 h at 25 deg C
Breakaway torque18.2N mISO 10964; degreased 3/8 x 16 steel; cured 72 h at 25 deg C
Prevail torque1.1N mISO 10964; degreased 3/8 x 16 steel; cured 72 h at 25 deg C
Breakloose torque27.9N mISO 10964; pretorqued 5 N m; degreased 3/8 x 16 steel; cured 72 h at 25 deg C
Breakloose torque18.5N mISO 10964; pretorqued 5 N m; phosphate-and-oil fasteners as received; cured 72 h at 25 deg C
Prevail torque2.5N mISO 10964; pretorqued 5 N m; phosphate-and-oil fasteners as received; cured 72 h at 25 deg C