LOCTITE 2422

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 2422 LOCTITE 2422

Main features

  • High-Temperature Threadlocking Paste
  • Thixotropic Paste Application
  • Serviceable Medium-Strength Locking

Product Description

LOCTITE 2422 is a blue, one-component anaerobic threadlocker paste for medium-strength locking and sealing of metal fasteners that must remain serviceable with hand tools. Its high thixotropic viscosity keeps the paste on threaded parts during application. It is used on less-active substrates, including stainless steel and plated surfaces, and in assemblies requiring elevated-temperature resistance. LOCTITE 2422 cures without air between close-fitting metal threads. Torque performance is specific to the defined steel fastener configurations, cure times, and pretightening conditions used for removable threaded assemblies.

Key features

  • High-temperature positioning: The threadlocker is intended for assemblies requiring elevated-temperature resistance.
  • Thixotropic paste control: High viscosity helps the product remain on threaded parts during application.
  • Serviceable medium strength: Cured assemblies are intended for disassembly with standard hand tools.

Applications / Suitable for

  • Removable locking and sealing of threaded metal fasteners
  • Stainless steel and plated fastener assemblies
  • Elevated-temperature threaded assemblies
Product Family

LOCTITE 2422

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
paste
Chemistry Type
Dimethacrylate ester
Color
Blue
Component System
1K
Specific Gravity
1.07
Physical Properties
Viscosity
35,000 to 80,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
AppearanceBlue paste-Uncured
ComponentsOne-No mixing required
Cure mechanismAnaerobic-Cures between close-fitting metal surfaces without air
Specific gravity1.18-Typical at 25 deg C
Viscosity35,000 to 80,000mPa sCone and plate; 50 mm parallel plates; 0.5 mm gap; 50 s^-1; 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakloose torque7.9 to 28.4N mISO 10964; pretorqued 5 N m; 3/8 x 16 degreased grade 5 steel; cured 24 h at 22 deg C
Breakaway torque11.6N mISO 10964; 3/8 x 16 degreased steel; cured 72 h at 22 deg C
Prevail torque1.4N mISO 10964; 3/8 x 16 degreased steel; cured 72 h at 22 deg C
Breakloose torque15.5N mISO 10964; pretorqued 5 N m; 3/8 x 16 degreased steel; cured 72 h at 22 deg C
Breakloose torque12.4N mISO 10964; phosphate and oil fasteners as received; cured 72 h at 22 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers