LOCTITE 222MS

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 222MS LOCTITE 222MS

Main features

  • Low-Migration Thixotropic Application
  • Easy Hand-Tool Disassembly
  • Small-Fastener Threadlocking Control

Product Description

LOCTITE 222MS is a purple, low-strength thixotropic anaerobic threadlocker for metal fasteners that require easy disassembly with standard hand tools. The one-component liquid cures when confined between close-fitting metal threads and does not require mixing before use. Its thixotropic flow helps reduce migration after application, making it useful for adjustment screws, small-diameter fasteners, and long threaded engagement. LOCTITE 222MS also fluoresces under UV light for application inspection. Torque ranges are specific to steel, cadmium-plated, and zinc-plated fastener configurations, with cure performance dependent on substrate, temperature, and joint conditions.

Key features

  • Low-migration flow: Thixotropic behavior helps the liquid remain at the applied thread area.
  • Easy disassembly: Low cured strength supports removal with standard hand tools.
  • Small-fastener control: The formulation is suited to adjustment screws and long-engagement fasteners.

Applications / Suitable for

  • Adjustment and set screws
  • Small-diameter metal fasteners
  • Long-engagement fasteners requiring hand-tool disassembly
Product Family

LOCTITE 222MS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Dimethacrylate ester
Color
Purple
Component System
1K
Specific Gravity
1.05
Physical Properties
Viscosity
800 to 1,600 mPa.s
Thermal Properties
Specific Heat Capacity
300 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
AppearancePurple liquid-Uncured
ComponentsOne-No mixing required
Cure mechanismAnaerobic-Cures between close-fitting metal surfaces without air
Specific gravity1.05-Typical at 25 deg C
Viscosity>=5,000mPa sBrookfield RVT, spindle 3, 2 rpm, Helipath, 25 deg C
Viscosity800 to 1,600mPa sBrookfield RVT, spindle 3, 20 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakaway torque3 to 9N mISO 10964; M10 steel nuts and bolts; cured 24 h at 22 deg C
Prevail torque1 to 6N mISO 10964; M10 steel nuts and bolts; cured 24 h at 22 deg C
Breakloose torque8 to 20N mISO 10964; M10 steel; pretorqued; cured 24 h at 22 deg C
Coefficient of thermal expansion80 x 10^-6K^-1ISO 11359-2; cured material
Thermal conductivity0.1W/(m K)ISO 8302; cured material
Specific heat0.3kJ/(kg K)Cured material