LOCTITE 087

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 087 LOCTITE 087

Main features

  • High-Strength Coarse-Thread Retention
  • 11.3 to 28.3 N m Prevail Torque
  • One-Part Heat-Assisted Disassembly

Product Description

LOCTITE GRD AV High-Strength Threadlocker is a one-part red anaerobic liquid for locking and sealing large, coarse-threaded nuts, bolts, and studs. Its 100 to 250 mPa s viscosity supports controlled application before assembly, and the high-strength cured bond is intended for fasteners requiring durable retention. After 24 hours at 22 deg C, it develops 7 N m breakaway torque and 11.3 to 28.3 N m prevail torque on 3/8 x 24 grade 2 steel fasteners under ISO 10964 testing. The product requires no mixing; disassembly is performed with localized heat when removal is necessary. Applications include large coarse-threaded metal assemblies where high locking strength is required.

Key features

  • High-Strength Coarse-Thread Locking: The red anaerobic liquid is intended for large coarse-threaded fasteners requiring high locking strength.
  • 11.3 to 28.3 N m Prevail Torque: Typical prevail torque is measured after 24 hours at 22 deg C on grade 2 steel fasteners.
  • Heat-Assisted Disassembly: Localized heat enables removal when the high-strength threaded assembly must be disassembled.

Applications / Suitable for

  • Large coarse-threaded nuts, bolts, and studs
  • High-strength metal fastener retention
  • Threaded assemblies requiring locking and sealing
Product Family

LOCTITE 087

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Dimethacrylate ester
Color
Red
Component System
1K
Specific Gravity
1.07
Physical Properties
Viscosity
100 to 250 mPa.s
Thermal Properties
Specific Heat Capacity
300 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
9.8 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and storage properties for LOCTITE GRD AV.

Property Value Unit Method / condition
Appearance Red liquid Uncured material; LMS
Components One component No mixing required
Viscosity 100 to 250 mPa s Cannon-Fenske; ISO 3104; uncured material
Specific gravity 1.07 At 25 deg C; uncured material
Cure mechanism Anaerobic Threadlocking application
Optimal storage 8 to 21 deg C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material and threaded-fastener results for LOCTITE GRD AV.

Property Value Unit Method / condition
Breakaway torque 7 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Prevail torque 11.3 to 28.3 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Dielectric breakdown strength 9.8 kV/mm IEC 60243-1; cured material
Thermal conductivity 0.1 W/(m K) ISO 8302; cured material
Coefficient of thermal expansion 100 x 10^-6 K^-1 ISO 11359-2; cured material
Specific heat 0.3 kJ/(kg K) Cured material