LOCTITE 084

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 084 LOCTITE 084

Main features

  • Low-Viscosity Thread Application
  • 6 N m Breakaway Torque
  • Medium-Strength Hand-Tool Removal

Product Description

LOCTITE 84 Medium-Strength Threadlocker is a one-part blue low-viscosity anaerobic liquid for locking and sealing fine-threaded nuts, bolts, and studs. Its 10 to 25 mPa s viscosity supports application to close-fitting threads and preassembled through-hole joints, while the medium-strength cured bond remains removable with ordinary hand tools. The material requires no mixing and cures after air is excluded within the threaded assembly. After 24 hours at 22 deg C, it develops 6 N m breakaway torque on 3/8 x 24 grade 2 steel fasteners under ISO 10964 testing. Applications include fine-threaded metal assemblies requiring secure retention and planned disassembly.

Key features

  • 10 to 25 mPa s Viscosity: The low-viscosity liquid supports application to fine threads and preassembled through-hole joints.
  • 6 N m Breakaway Torque: Typical breakaway torque is measured after 24 hours at 22 deg C on grade 2 steel fasteners.
  • Hand-Tool Removable Strength: The medium-strength cured assembly can be removed with ordinary hand tools.

Applications / Suitable for

  • Fine-threaded nuts, bolts, and studs
  • Preassembled threaded parts with through holes
  • Metal fastener locking and sealing
Product Family

LOCTITE 084

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Dimethacrylate ester
Color
Blue
Component System
1K
Specific Gravity
1.05
Physical Properties
Viscosity
10 to 25 mPa.s
Thermal Properties
Specific Heat Capacity
300 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
9.8 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and storage properties for LOCTITE 84.

Property Value Unit Method / condition
Appearance Blue liquid Uncured material; LMS
Components One component No mixing required
Viscosity 10 to 25 mPa s Cannon-Fenske; ISO 3104; uncured material
Specific gravity 1.05 At 25 deg C; uncured material
Cure mechanism Anaerobic Threadlocking application
Optimal storage 8 to 21 deg C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material and threaded-fastener results for LOCTITE 84.

Property Value Unit Method / condition
Breakaway torque 6 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Prevail torque 4.5 to 11.3 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Dielectric breakdown strength 9.8 kV/mm IEC 60243-1; cured material
Thermal conductivity 0.1 W/(m K) ISO 8302; cured material
Coefficient of thermal expansion 100 x 10^-6 K^-1 ISO 11359-2; cured material
Specific heat 0.3 kJ/(kg K) Cured material