LOCTITE 083

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 083 LOCTITE 083

Main features

  • Medium-Strength Hand-Tool Removal
  • 8 N m Breakaway Torque
  • Controlled One-Part Application

Product Description

LOCTITE GRD CV Medium-Strength Threadlocker is a one-part blue anaerobic liquid for locking and sealing fine-threaded nuts, bolts, and studs. Its 100 to 250 mPa s viscosity supports controlled placement on threaded metal assemblies, while the medium-strength cured bond allows removal with standard hand tools. The material requires no mixing and cures after assembly when confined between close-fitting metal surfaces. After 24 hours at 22 deg C, it develops 8 N m breakaway torque on 3/8 x 24 grade 2 steel fasteners under ISO 10964 testing. Applications include fine-thread fasteners that need secure retention with planned service access.

Key features

  • 8 N m Breakaway Torque: Typical breakaway torque is measured after 24 hours at 22 deg C on grade 2 steel fasteners.
  • Medium-Strength Serviceability: The cured assembly can be removed with standard hand tools.
  • Controlled One-Part Viscosity: The 100 to 250 mPa s liquid requires no mixing before application.

Applications / Suitable for

  • Fine-threaded nuts, bolts, and studs
  • Threaded assemblies requiring hand-tool removal
  • Metal fastener locking and sealing
Product Family

LOCTITE 083

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Liquid
Chemistry Type
Dimethacrylate ester
Color
Blue
Component System
1K
Specific Gravity
1.05
Physical Properties
Viscosity
100 to 250 mPa.s
Thermal Properties
Specific Heat Capacity
300 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
9.8 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and storage properties for LOCTITE GRD CV.

Property Value Unit Method / condition
Appearance Blue liquid Uncured material; LMS
Components One component No mixing required
Viscosity 100 to 250 mPa s Cannon-Fenske; ISO 3104; uncured material
Specific gravity 1.05 At 25 deg C; uncured material
Cure mechanism Anaerobic Threadlocking application
Optimal storage 8 to 21 deg C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material and threaded-fastener results for LOCTITE GRD CV.

Property Value Unit Method / condition
Breakaway torque 8 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Prevail torque 4.5 to 11.3 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Dielectric breakdown strength 9.8 kV/mm IEC 60243-1; cured material
Thermal conductivity 0.1 W/(m K) ISO 8302; cured material
Coefficient of thermal expansion 100 x 10^-6 K^-1 ISO 11359-2; cured material
Specific heat 0.3 kJ/(kg K) Cured material