LINQSOL EMC-G833 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LINQSOL EMC-G833 | Black Epoxy Mold Compound

Main features

  • Green epoxy molding compound
  • Designed for Quad Flat No Leads(QFN), Quad Flat (QFP) packages and DFN Packages
  • Excellent reliability performance

Product Description

LINQSOL EMC-G833  is a green epoxy molding compound specifically developed for the encapsulation of Quad Flat No Leads(QFN), Quad Flat (QFP) packages and other surface mount packages. Its wide gel time provides a better processing window, required for QFN, DFN nd QFP molding.  

LINQSOL EMC-G833 has a high spiral flow that meets higher flowability requirements. Additionally, with a UL 94 V-0 flammability rating and ultra-low water absorption, EMC-G833  guarantees excellent performance and outstanding reliability. This product is deliberately formulated without the inclusion of substances prohibited by the European Union RoHS and REACH.  

Overall, LINQSOL EMC-G833  seamlessly integrates advanced material properties, safety compliance, and superior performance to deliver a reliable solution for semiconductor device encapsulation.

 

Available Variants

  • LINQSOL EMC-G833  Standard Epoxy Mold compound for MSL 3 QFN, DFN and QFP. 
  • LINQSOL EMC-G833R MSL 1 Capable

 

Reliability Tests Passed:

  • Preconditioning: 30°C, 60% RH
  • u-HAST: T=130°C, RH= 85%, P= 230kPa
  • PCT, Tₐ=121°C, P=205 kPa, RH=100%* 168 hours
  • TCT, –65 to 150 °C * 1000 cycles
  • HTST, T=150°C  * 1000 hours
Product Family

LINQSOL EMC-G833

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
87 %
Specific Gravity
1.97
Thermal Properties
Glass Transition Temperature (Tg)
112 °C
UL 94 Rating
V-0
Physical Properties
Spiral Flow @ 175°C
165 cm
Curing Conditions
Transfer Pressure
70-150 kg/cm2
Transfer Time
8-25 s

Additional Information

 

LINQSOL EMC-G833 Series Product Property Comparison

 
PROPERTY UNIT EMC-G833 EMC-G833R

Color

–

Black

Black

Filler content

%

87

88

Filler cut size

µm

75

75

Specific gravity

–

1.97

2.0

Spiral flow at 175 °C

cm

165

150

Ion content

Chloride (Cl–) concentration

Sodium (Na+) concentration


ppm

ppm


7

6

5

5

Electrical conductivity of extract

µS⋅cm–1

50

30

Flexural strength

MPa

145

162

Flexural modulus

GPa

22.8

24

Glass transition temperature

°C

112

118

Coefficient of thermal expansion, α1

ppm/K

11

10

Coefficient of thermal expansion, α2

ppm/K

36

36

Gel time at 175 °C

sec

57

52

Flammability

UL-94

V-0

V-0

 

 

LINQSOL EMC-G833 Storage and Handling

LINQSOL EMC-G833 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life when stored below 5 °C is 183 days.

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

 

Presentations

Ball Grid Array and Land Grid Array Packages

The presentation above shows the materials used for Ball Grid Array and Land Grid Array Packages.

Quad Flat No Lead and Dual Flat No Lead Packages

The presentation above shows the materials used for Quad Flat No Lead and Dual Flat No Lead Packages.

EMC-G833 MSL 3 Reliability Test Data

This presentation summarizes the reliability performance of EMC-G833 under MSL 3 test conditions.