LINQSOL EMC-G135 is a green epoxy molding compound specifically developed for rectifier bridges (GBU, KBJ, GBS and etc.) and SMX packages. It offers good moldability and low modulus to meeting low-stress requirements. With a thermal conductivity of ~1.7W/m⋅K, it satisfies the heat dissipation required by high-performing packages. G135 boasts of its high-cost effectiveness and excellent workability with more than 500 continuous mold shots. 

LINQSOL EMC-G135 guarantees strong performance and outstanding reliability. This product is deliberately formulated without the inclusion of substances prohibited by the European Union RoHS and REACH. Overall, LINQSOLTM EMC-G135 seamlessly integrates advanced material properties, safety compliance, and superior performance to deliver a reliable solution for semiconductor device encapsulation.

Key Features

  • ~1.7 W/m·K thermal conductivity — Enhances heat spreading in high-current bridge rectifiers.
  • Low modulus (~16 GPa) — Reduces package stress and risk of crack/warp during cycling.
  • High moldability (spiral flow ~88 cm) — Fills complex cavities cleanly; supports small gates and long runners.
  • 500+ continuous shots — Stable release and low bleed for fewer interruptions and lower scrap.
  • Electrical cleanliness (Cl⁻ ~9 ppm, Na⁺ ~4 ppm) — Minimizes ionic pathways that can lead to leakage or corrosion.
  • Low moisture uptake (~0.45% PCT 24 h) — Helps maintain insulation and dimensional stability.
  • UL-94 V-0 flammability — Meets stringent safety requirements for power electronics.
  • RoHS/REACH compliant — Free from substances of concern for global market access.

Reliability Tests Passed:

  • HTRB, Tₐ=125°C, V=80%VR * 500 hour
  • PCT, Tₐ=121°C, P=0.215atm, RH=100%* 98 hours
  • Thermal Cycling Test, -55°C - +150°C * 500 cycles

Application/Suitable For:

  • Bridge rectifier packages: GBU, KBJ, GBS; SMX packages
  • AC/DC power supplies, chargers, UPS rectifier stages
  • Motor drives and industrial controls (bridge diode modules)
  • General power conversion, where thermal conductivity and low package stress are critical

 

Product Family

LINQSOL EMC-G135

1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Package Type, Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
76.5 %
Specific Gravity
2.0
Thermal Properties
Glass Transition Temperature (Tg)
160 °C
Thermal Conductivity
1.7 W/m.K
UL 94 Rating
V-0
Electrical Properties
Volume Resistivity
6E15 Ohms⋅cm
Chemical Properties
Moisture absorption
0.45 %
Physical Properties
Spiral Flow @ 175°C
88 cm
Curing Conditions
Transfer Pressure
40-70 kg/cm2
Transfer Time
17-25 s

Additional Information

 Processing Instructions

  • Before use, let LINQSOL EMC-G135 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 

  • Use the materials within 72 hours after removing the container from cold storage.

 

Storage and Handling

 LINQSOL EMC-G135 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days. 

 

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers