LINQSOL EMC-7535 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

EMC-7535 | Black Epoxy Mold Compound

Main features

  • Green molding compound
  • Designed for high-power TO packages
  • High Tg, low water absorption, low modulus, and excellent thermal stability

Product Description

LINQSOL EMC-7535 is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 175 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating,  EMC-7535 guarantees strong performance and outstanding reliability.

Overall, LINQSOL EMC-7535 seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages.

Product Family

LINQSOL EMC-7535

1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type, Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
black
Filler Content
75 %
Specific Gravity
1.96
Electrical Properties
Volume Resistivity
16000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.25 %
Physical Properties
Spiral Flow @ 175°C
86 cm
Thermal Properties
Glass Transition Temperature (Tg)
175 °C
UL 94 Rating
V-0
Mechanical Properties
Molded Shrinkage
0.1 %
Curing Conditions
Transfer Pressure
40-90 kg/cm2
Transfer Time
10-25 s

Additional Information

Processing Instructions

  • Before use, let LINQSOL EMC-7535 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 
  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7535 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.