LINQSEAL GS-EPDM

Harmonization Code : 4016.93 | Gaskets, washers and other seals made from vulcanized rubber

LINQSEAL EPDM

Main features

  • Low cost sealing solution
  • High hear resistance and tensile strength
  • High water (steam) resistance

Product Description

LINQSEAL GS-EPDM gaskets consist primarily of ethylene (comprising 45–75%), along with propylene and diene monomers. This unique composition provides the gaskets with exceptional versatility and durability. The diene monomers contribute to the formation of a cross-linking structure, enhancing the mechanical properties, such as elasticity, and significantly increasing resistance to aging. This rubber material exhibits high resistance to a wide range of environmental factors, including heat, cold, ozone, steam, electricity, UV rays, abrasion, and water, making it a preferred choice for various outdoor and challenging conditions. Compared to silicone and other polymers, EPDM boasts a higher tensile strength. Overall, LINQSEAL GS-EPDM is a cost-effective solution with outstanding performance in demanding outdoor environments.

Custom LINQSEAL GS-EPDM gaskets can be tailored precisely to your specifications and drawings. The thickness ranges from 0.5 to 5.0 millimeters. The maximum dimensions are 1500 × 1500 mm2, while the minimum dimensions are 100 × 100 mm2.

Key Features:

  • High tensile strength
  • High abrasion and weather resistance
  • Good temperature stability (–57 °C to 150 °C)

Highly Recommended As:

 

Product Family

LINQSEAL GS-EPDM

1. Select Package Type
2. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1.45–1.50 g/cm3
Thermal Properties
Operating Temperature
–57 to 150 °C
Mechanical Properties
Elongation
200 %