LINQCELL GDP210 | 210um Non woven Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDS210 | 210um Carbon Paper GDP210 | 210um Carbon Paper

Main features

  • 0.21mm - 210um - 8.2mil
  • Non woven
  • Roll form is possible.

Product Description

LINQCELL GDP210 is a 0.21mm thick non woven carbon paper without a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less than 10 mΩcm2. This carbon paper is highly flexible and has excellent air permability.

LINQCELL GDP210 is a close alternative to the discontinued Spectracarb 0850. It is one of the few products that come in long roll form.

Product Family

LINQCELL GDP210

1. Select Sheet Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Sheet Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
50 g/m2
Other Properties
Air Permeability
10 seconds
Mechanical Properties
Tensile Strength (Thin Film)
2 N/cm

Additional Information

LINQCELL GDP210 Properties

Property Value Unit
Thickness at 50 kPa 0.21 mm
Basis Weight 51 g/cm2
Air Permeability 3.3 s
Through-plane Resistance 10 mΩ⋅cm2
Voltage 14 mV

 