LINQCELL GDP090 | 90um Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDP090 | 90um Carbon Paper

Main features

  • Ultra-thin thickness (0.09 mm - 90 µm - 3.54 mil)
  • High graphitization temperature (2000 °C)
  • Optimized as gas diffusion layers in fuel cells

Product Description

LINQCELL GDP090 is an ultrathin, 90-µm thick graphitized carbon fiber paper without a microporous layer, made from high-quality polyacrylonitrile (PAN) fibers. The fibers undergo a wet-laying paper process to form a non-woven, fibrous, and porous structure, which is then carbonized and graphitized at an exceptionally high temperature of 2000 °C. This high graphitization temperature significantly improves electrical conductivity, thermal stability, and oxidation resistance.

Key Features:

  • Ultra-thin Profile: At just 90 µm (0.09 mm), GDP090 minimizes stack volume, enabling compact fuel cell designs without compromising performance.
  • High-Temperature Graphitization: Graphitized at an elevated temperature of 2000 °C, this carbon fiber paper has a highly-crystalline graphite-like structure, enhancing conductivity, thermal stability, and oxidation resistance for demanding applications.
  • No MPL and PTFE Layer: Enables direct control of interfacial modifications for system-specific optimization in fuel cells and electrochemical devices.

The improved properties of LINQCELL GDP090 make it highly suitable for use as anode and cathode gas diffusion layers in fuel cells. Its ultra-thin design reduces stack volume, enhancing overall fuel cell efficiency by minimizing internal resistance. Additionally, its low thickness combined with high permeability makes it ideal for high humidity fuel cell operation (≥60%) at temperatures between 50 to 80°C. In medium humidity conditions (20 to 60%), LINQCELL GDP090 performs effectively at lower temperatures (≤50°C), covering stable and efficient fuel cell operation across a wide range of humidity and temperature conditions.

Highly Recommended As:

Recommended For Fuel Cells Operating at:

  • High humidity (≥60%) at temperatures between 50 to 80 °C
  • Medium relative humidity (20 to 60%) at low temperatures ≤50 °C
Product Family

LINQCELL GDP090

1. Select Sheet Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Sheet Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
55 g/m2
Porosity
68 %
Electrical Properties
TP Resistance
6 mΩcm2
Voltage loss
7 mV
Other Properties
Air Permeability
50 seconds
Mechanical Properties
Tensile Strength (Thin Film)
15/10 (MD/XD) N/cm