LINQCELL CF350 | 350um Carbon Fabric

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL CF350 | 350um Carbon Fabric

Main features

  • 0.35mm - 350um - 14mil
  • Comes in roll form
  • 5 TP Resistance

Product Description

LINQCELL CF350 is a 0.35mm thick carbon cloth without a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less rhN 5 mΩcm2.

LINQCELL CF350 carbon cloth is typically used in PEM fuel cells as well as Phosphoric acid fuel cells and Direct methanol fuel cell applications as a gas diffusion layer. Carbon cloth based GDLs have performance equal to that of conventional carbon papers. Carbon cloth is more practical than carbon paper because of its superior compressibility, elasticity, and flexibility performance, making it more appropriate for ongoing manufacturing and assembly processes. 

These thinner gas diffusion layers lend themselves better to AEMFC GDL Anodes. Thickness has more sensitivity to the AEMFC when used in the anode electrode rather than in the cathode electrode, indicating that water removal at the anode was more challenging than water supply at the cathode so the strategy of water management among electrodes should be differentiated.

Product Family

LINQCELL CF350

1. Select Sheet Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Sheet Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
130 g/m2
Total Thickness
360 μm
Electrical Properties
TP Resistance
5 mΩcm2
Mechanical Properties
Tensile Strength (Thin Film)
10 N/cm

Additional Information

Please note that the thickness can easily vary ±10-20um