LINQBOND PM-4911 | Two part silicone potting material

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

OPTOLINQ PM-4911 | Two part silicone potting material

Main features

  • Low stress silicone potting gel
  • Low viscosity, good leveling, and bubble-free curing
  • Excellent long term temperature resistance

Product Description

LINQBOND PM-4911 is a two-component, low-stress transparent packaging adhesive. When the two components are mixed in a 1:1 ratio (by volume), they cure into a soft silicone gel. This gel offers buffering, shock absorption, insulation, waterproofing, and moisture-proof functions for electronic components. With a very low modulus, it generates minimal internal stress and exhibits robust resistance to cold and heat shock.

LINQBOND  PM-4911 also exhibits excellent adhesion on various surfaces, making its suitable for insulating a wide array of electronic components. PM-4911 is an ideal potting material for IGBTs, displays, and precision components.

Product Family

LINQBOND PM-4911

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
1:1
Pot Life
2 hours
Electrical Properties
Volume Resistivity
1000000000000000 Ohms⋅cm

Additional Information

Premixed Properties

Property

Part A

Part B

Appearance

Transparent

Transparent

Density [g/cm3]

0.92-1.02

0.92-1.02

Viscosity [cP]

400-500

250-350

Precautions before Use

  1. Avoid contact with condensed silicone rubber, its gas, nitrogen, sulfur, phosphorus, and other chemicals, including heavy metals, as they may inhibit curing of the product.
  2. Maintain a clean and ventilated workplace, using extraction trunks when necessary.
  3. Wear appropriate protective equipment and minimize direct contact with the human body. Refer to the Material Safety Data Sheet (SDS) before use.

Storage and Handling

Store in a well-ventilated, dry area below 25 °C, away from fire and heat sources. Avoid outdoor storage. For extended shelf life, consider cold storage. Shelf life is 12 months under recommended conditions.

 