LINQBOND PM-1221 | Two part polyurethane potting material

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

OPTOLINQ PM-1221 | Two part polyurethane potting material

Main features

  • Low-stress potting material
  • Excellent seismic and voltage resistance
  • Room temperature curing

Product Description

LINQBOND PM-1221 is a two-component polyurethane potting material engineered for low-stress applications. It offers good insulating properties and exceptional high-temperature, shock, and voltage resistance. With its excellent fluidity during application and minimal bubble formation upon curing, LINQBOND PM-1221 seamlessly integrates into your projects, ensuring a smooth and reliable finish.

LINQBOND PM-1221 is the ideal choice for casting bonding, and sealing electronic components operating in challenging environments such as high pressure, high frequency, humidity, and heat. It is perfectly suited for precision arresters, various transformers, filters, control boards, and igniters. LINQBOND PM-1221 viscosity can be customized according to customer requirements. Other available colors can be found in the selector guide below.

 

Available Versions

  • LINQBOND PM-1221: Precision Bonding with Low-Stress Protection (STD)

  • LINQBOND PM-1221 Type E: High-Hardness Epoxy Replacement

  • LINQBOND PM-1221 Type M: Multi-Function Environmental Sealant

  • LINQBOND PM-1221 Type S: Flexible, Repairable Silicone Alternative

  • LINQBOND PM-1221 Type F Adhesive: Precision Bonding for Electronic Components

 

 

 

Product Family

LINQBOND PM-1221

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Polyurethane
Mix Ratio
5:1
Pot Life
0.75 hours
Specific Gravity
1.5–1.7
Thermal Properties
Operating Temperature
–60 to 150 °C
Thermal Conductivity
≥0.6 W/m.K
UL 94 Rating
V-0
Electrical Properties
Dielectric Strength
≥25 kV/mm
Volume Resistivity
1.0 × 10¹⁵ Ohms⋅cm
Chemical Properties
Moisture absorption
0.2 %

Additional Information

LINQBOND PM-1221 Polyurethane Potting and Adhesive Solutions

Unmatched Protection, Durability, and Performance for Precision Electronics

Discover the PM 1221 series—a high-performance line of polyurethane potting and adhesive solutions tailored to meet the unique demands of sensitive electronic components, from precision capacitors to transformers, control boards, and more. Designed to outperform standard materials, each formulation in the PM 1221 range delivers specific features that address key performance needs, offering robust protection with specialized functionality.

 

LINQBOND PM-1221 Polyurethane Potting Sealant: Precision Bonding with Low-Stress Protection

This all-in-one potting sealant excels in low-stress, seismic-resistant applications, ensuring long-lasting integrity under electrical, mechanical, and environmental pressures. Specifically designed for arresters, transformers, filters, and control boards, it boasts excellent electrical insulation and resistance to vibration, delivering an ideal solution for components in high-performance environments.

Key Benefits

  • Low-Stress, Seismic-Resistant: Reduces risk of component fatigue
  • Superior Electrical Properties: Optimal for voltage-intensive applications
  • Versatile Compatibility: Bonds with a wide range of electronic components

 

LINQBOND PM-1221 Type E: High-Hardness Epoxy Replacement

Engineered with high hardness and durability, PM 1221 Type E is the go-to choice for applications requiring a firm, resilient bond. Ideal for potting precision capacitors, this sealant provides a stable alternative to traditional epoxy with greater ease of handling. When used with vacuum deaeration and heating equipment, it cures to a dense, rigid form with minimal bubbles—perfect for reinforcing and safeguarding intricate components.

Key Benefits

  • High Hardness: Perfect for high-stress environments
  • Epoxy Alternative: A cleaner, versatile substitute
  • Precision Protection: Formulated for high-performance capacitors

LINQBOND PM-1221 Type M: Multi-Function Environmental Sealant

Purpose-built for environmental durability, PM 1221 Type M ensures electronics remain insulated, waterproof, and shockproof, even in challenging conditions. It’s the ultimate choice for protecting devices from moisture, dust, and other environmental hazards, providing complete peace of mind in a single potting and sealing solution.

Key Benefits

  • Comprehensive Protection: Moisture-proof, shockproof, and waterproof
  • Environmental Resilience: Seals against air, moisture, and external elements
  • Broad Application: Suitable for diverse electronic assemblies

 

LINQBOND PM-1221 Type S: Flexible, Repairable Silicone Alternative

With unmatched elasticity and toughness, PM 1221 Type S offers a repairable, highly flexible sealant ideal for applications requiring both durability and the option to make modifications. This type outperforms traditional silicone potting in electrical properties, offering enhanced flexibility without compromising performance.

Key Benefits

  • Repairable Flexibility: Adaptable for evolving project needs
  • High Elasticity and Toughness: Ensures long-term durability
  • Silicone Replacement: Enhanced electrical performance with flexible rework options

 

LINQBOND PM-1221 Type F Adhesive: Precision Bonding for Electronic Components

Semi-flowing for easy application, PM 1221 Type F adhesive offers robust bonding and sealing for electronic components where precision matters most. It delivers a strong, lasting hold that withstands the demands of high-performance applications.

Key Benefits

  • Semi-Flowing Application: Easy handling for precision bonding
  • Reliable Adhesion: Ideal for secure bonding in sensitive electronics
  • Optimized for Electronics: Designed specifically for electronic components

Experience the next level of electronic protection and performance with PM 1221’s tailored polyurethane solutions.

 

Properties PM-1221 PM-1221 Type E PM-1221 Type M PM-1221 Type S PM-1221 Type F
Part A Appearance Transparent, White Gray, Black Liquid
Part B Appearance Light Yellow Liquid
Part A Viscosity 6,000-9,000 20,000
Part B Viscosity 300-400 400
Mixed Viscosity 3,000- 5,000 10,000-15,000
Pot Life 30-45 ≤30 45-60 45-60 ≤30
Initial Curing Time 5-7 3-5 8-10 8-10 3-5
Full Cure Time 36 24 48 48 24
Shore Hardness 70-90 Shore A ≥80 Shore D 50-70 Shore A 30-50 Shore A ≥80 Shore D
Shear Strenght ≥2.3 ≥3.5 ≥1.5 ≥0.8 ≥4.8
Specific Gravity 1.5 -1.7
Linear Shrinkage Rate 0.3
Working Temperature Range -60 up to 150
Dielectric Strenght ≥25
Volume Resistance     1.0E15    
Thermal Conductivity ≥0.6

 

 

Processing Instructions

  1. Mix component A and B according to specified ratio. Stir thoroughly to ensure uniformity while preventing air to be introduced into the mixture.
  2. Degas the mixture to remove the bubbles for about 5 minutes. Do not fill the container more than half full to prevent overflowing during degassing.
  3. Gradually pour the mixed compound into the device being potted. If the ambient temperature is around 5 °C, preheat components A and B to around 15 °C.
  4. Allow the potted workpiece cure at room temperature until the surface is dry. Full curing typically occurs within 24 hours. The curing process is influenced by temperature variations; generally, higher temperatures result in faster curing, while lower temperatures lead to slower curing.

Precautions for Use

  1. Use the mixture promptly after combining components A and B to prevent a significant increase in viscosity.
  2. If the components have been stored for an extended period and exhibit precipitation or stratification, they should be thoroughly mixed before use. Component B is prone to crystallization at low temperatures; therefore, it should be stored in a warmer environment to melt prior to use, ensuring product performance remains unaffected.

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

Storage and Handling

Store in a ventilated, dry, and clean environment below 25 °C and  50% RH. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A and Part B has a shelf life of 6 months. Shelf life can be extended by using cold storage.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers