LINQALLOY SP-SAC0307 | Solder paste

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

LINQALLOY SP-SAC0307 | Solder paste

Main features

  • Sn99Ag0.3Cu0.7 Alloy
  • 217 - 228°C
  • Powder size: T3, T4 and T5

Product Description

LINQALLOY SP-SAC0307 is a lead free, no clean, solder paste, comprised of 99% tin, 0.3% silver, 0.7% copper that has been designed for Surface Mount Technology(SMT). No-Clean Solder Paste is designed for applications where post-soldering cleaning is unnecessary, providing minimal, non-conductive residues.

LINQALLOY-SP-SAC0307 solder paste is crafted with refined tin powder that allows for exceptional printing capabilities and minimal oxide content. This solder paste has enhanced flux content (higher %) that guarantees higher reliability. With its low iconic activator system it leaves behind minimal residues post reflow resulting in exceptionally high insulation resistance and excellent reliability

Product Family

LINQALLOY SP-SAC0307

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
190 - 230 mPa.s
General Properties
Alloy Type
SAC0307