Product Description

LINQSTAT VCF-8S200K is a black, carbon-filled, electrically conductive polyethylene plastic film designed to provide both physical and static protection. Having a surface resistance of 200,000 ohm-sq, (2x105 Ω-sq) it offers medium-level static protection which means it effectively avoids accumulation of electric charge on itself and the products which it protects. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. Please note that this film is only surface conductive and not volume conductive.

VCF-8S200K is useful in applications where the key is to balance cost versus performance. As a medium-level conductive plastic, the carbon-loading is such that it is low-enough to be cost-effective, while being high enough to meet the electrical requirements of military specification MIL-PRF-81705D Type II and MIL-P-82646A. It is typically used as an antistatic smartcard interleaver.

VCF-8S200K film and its conductivity are unaffected by humidity and age. The film is heat-sealable, flexible and offers exceptional abrasion resistance. The film gives good thermal stability and has outstanding chemical resistance. It has a standard thickness of 8mil(0.2mm) is available in sheeting, tubing, V-fold and C-fold versions. Roll lengths and widths vary depending on thickness and application.

Production batches from 2023 will have a Tolerance of ±100,000 ohms

Product Family

LINQ VCF-8S200K

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Carbon-Loaded PE
Color
Black
Film Thickness
0.2 mm
Specific Gravity
1.02-1.10
Electrical Properties
Surface Resistivity
200000 Ohms/sq
Other Properties
RoHS Compliant
Yes

Additional Information

In sheet form, LINQSTAT VCF, works as an antistatic plastic. For more sensitive pressure sensor applications, KRAYDEN recommends LINQSTAT XVCF-Series, which is a more-conductive series of polyethylene plastics. As an antistatic packaging plastic, it is also used as a antistatic interleaver for Smartcard (micromodule) applications to separate subsequent layers of smartcard chips in micromodule production. 

 

Product Applications

  • Protection and storage of static-sensitive components
  • Interleaf between rolls of Smartcard modules
  • Grounding Mats

Product Features and Benefits

  • Volume-conductive plastic
  • Black Opaque - Printable
  • Provides Anti-Static protection to electronics components
  • Groundable
  • Humidity independent conductivity
  • Meets military specification MIL-P-82646A

Chemical Susceptibility

  • Methanol: Resistant
  • Ethanol: Resistant
  • Isopropanol: Resistant
  • Weak Acids: Resistant
  • Ketones (Acetone): Slow Attack
  • Weak Alkalines: Slow Attack
  • Hydrocarbons: Non-Resistant

We have recently changed our SKUS. To help you search for them either on google or on our website here's a before and after table. As you can see we went for the "Product codes that make sense" approach:

VCF-80012S/2 VCF-8S200K/30CM-46M 30cm wide x 46m long

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers