TC-8020T | Optically Clear Molding Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features

  • LED Encapsulation
  • Optically clear
  • Emitter and Detector encapsulation

Product Description

OPTOLINQ TC-8020T is a high transmission, one component, optically clear epoxy molding compound that is specifically developed for emitter and LED encapsulation. Its excellent fluidity design aids it to become easily mouldable and processable while offering excellent package performance and durability. This is supported by its long term transmittance and post reflow reliability.

OPTOLINQ TC-8020T is a single component epoxy with superior adhesion performance, transmittance and stability at high temperatures. It is mainly utilised to package single color (monochrome) LEDs, 7-segment LED displays, compact LED indicators, monochrome ChipLEDs and photo-links.It offers good adhesion to Bismaleimide Triazine - BT substrates and metal leadframes, good flexural modulus, and excellent anti-reflow performance while also passing the stringent MSL 3/2A JEDEC requirements. Check TC-8020T Internal Reliability Test Results. 

Typical Applications

  • Low-Power LED & Emitters
  • Pulse Oximeter Sensors
  • Ambient Light Sensors
  • IR and Near-IR Sensors
  • Data transmission and industrial fibers.

Versions Available

Comparable With: XX-18, XX-8524, XX-330H

 

Product Family

LINQ TC8020T

1. Select Package Type
2. Select Pellet Size
3. Select Pellet Weight
4. Select Transmittance
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Package Type, Pellet Size, Pellet Weight and Transmittance.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.56
Specific Gravity
1.23
Mechanical Properties
Molded Shrinkage
1.6 %
Chemical Properties
Moisture absorption
0.45 %
Water Absorption
0.17 %
Curing Conditions
Transfer Pressure
10 - 40 kg/cm2
Transfer Time
20 - 50 s
Physical Properties
Spiral Flow @ 175°C
150 - 250 cm

Additional Information

 

TC8020 Series Product Properties Comparison

 
PROPERTY UNIT TC-8020T TC-8020L TC-8020LS TC-8020T-SR
Viscosity  cP 300 300 200 300
Spiral Flow @150°C cm 150-250 150-250 150-250 150-250
Hot Plate Gel Time @150°C sec 20-40 25-50 20-50 20-40
Glass Transition Temperature °C 125 115 95 125

CTE by TMA, α1

CTE by TMA, α2

ppm

ppm

70

170

70

170

70

220

70

170

Moisture Absorption PCT

24 hrs @25°C water

24 hrs @121°C, 2atm, 100%RH

 

wt%

wt%

 

0.17

3.2

 

0.16

3.2

 

0.17

3.8

 

0.17

3.2

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Mpa

130

3000

130

2900

110

3100

130

3000

yellowing Δb - 4 hrs @200°C

yellowing Δb - 30 min @280°C

yellowing Δb - 4 hrs UV

-

5

33

11

8

42

16.5

25

45

16.5

5

37

11

Transmittance 1mm @450nm % >90 >90 >90 >90
Refractive Index @633nm - 1.56 1.56 1.56 1.56
Comment   Standard Item for through-hole and surface mount component Low stress version for better reflow performance Low stress for balanced reflow and thermal shock test performance Self-release technology without compromising key properties
 

TC-8020T DSC & DMA Data 

TC-8020L/LS shows lower modulus at 150℃ and -50℃, which improves performance in thermal cycling and thermal shock tests.

TC8020T DSC CurveTC-8020T DSC Curve
TC-8020 DMA Storage ModulusTC-8020T DMA Data Curve
 

TC-8020T Optical Filter Choice

Transmittance wavelength window could be adjusted according to customers' specifications.

TC-8020 Cutoff Filter Versions Transmittance DataTransmittance Curve: TC-8020T Cutoff Filter 1mm
TC-8020 Bandpass Filter TransmittanceTransmittance Curve: TC-8020T Bandpass Filter 0.4mm

TC-8020T Reliability Test Results

 
Tests Test Conditions Electrical Test Yellowing
High Temperature Storage 200°C * 4 hr Pass Δb < 4.5
UV Exposure 25w * 1 hr @340nm Pass Δb < 12.0
Reflow 10 x 30 sec @ 260°C, IR reflow Pass Δb < 35.0
3 x 30 sec @ 260°C, IR reflow after 6 hrs' storage @85 °C and 85% RH Pass -
Thermal Shock 15 mins@-40°C ~ 15mins@100°C, 300 cycles Pass -
Red Dye Penetration PCT, 12 hrs @121°C Pass -
Double 85 168 hrs @85°C and 85% RH Pass -
High Temperature Storage 125°C * 500 hrs Pass -
HAST HAST 110; HAST 130 Pass -

Presentations

Clear Molding Compounds for Optoelectronic Applications

 

Sensing Applications Clear Molding Compounds

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers