Die Cut Kapton Tape on Release Liner PIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner PIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner PIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner PIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner 2-mil Polyimide (Kapton) Tape Silicone Adhesive Release Liner 2mil Polyimide High Temperature Dicing Tape | Release Liner Structure

Main features

  • 2 mil polyimide film
  • Silicone adhesive
  • >11000V breakdown voltage

Product Description

LINQTAPE™ PIT2S-RL-Series s is a high-temperature resistant polyimide tape on a 2 mil PET release liner. It is designed primarily for high temperature temporary bonding applications and it removes cleanly without adhesive residue after exposure to heat or chemicals. It may also be used in electrical insulation applications that require Class H tape grade.

LINQTAPE™ PIT2S-RL-Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 260°C (500°F).

LINQTAPE™ PIT2S-RL-Series comes as a standard in 36 yard (33m) lengths of varying widths, but longer rolls may be available upon request.

Product Family

LINQ PIT2S-RL

1. Select Width
2. Select Length
Price starting from $8.04
Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Silicone
Adhesive Thickness
38.1 µm
Chemistry Type
Polyimide
Color
Amber
Film Thickness
50.8 µm
Release Liner
Single Release Liner
Single or Double-Sided Adhesive
Single-Sided
Special Layer
None
Total Thickness
88.9 μm
Thermal Properties
Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage
>11000 V
Dielectric Strength
197 kV/mm
Volume Resistivity
10000000000000 Ohms⋅cm
Other Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength
26 Oz/in