PIT2A-LO | 2-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive
Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls
Main features
- 2 mil polyimide film
- Non-silicone, low outgassing acrylic adhesive
- 6,500 V breakdown voltage
Product Description
LINQTAPE™ PIT2A-LO is a Polyimide tape with 2mil backing thickness and 1.5mil acrylic adhesive with low outgassing. This tape has less than 1% TML and less than 0.1% CVCM values, making it suitable for aerospace applications.
LINQTAPE™ PIT2A-LO has good adhesion and tensile strength and can operate in temperatures between -29°C to 177°C.
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Temperature Resistance
177 ˚C
Electrical Properties
Breakdown Voltage
6,500 V
Mechanical Properties
Adhesion Strength
50 Oz/in
Elongation
55 %
Tensile Strength (Thin Film)
88 N/cm
General Properties
Adhesive Layer
Low Outgassing Acrylic
Adhesive Thickness
38.1 µm
Color
Amber
Film Thickness
50.8 µm
Release Liner
Paper
Total Thickness
88.9 μm