PIT1S-ESD-DCD | 1 mil Die Cut ESD Polyimide (Kapton) Tape with Silicone Adhesive | Single side Discs

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

1 mil Die Cut ESD Polyimide Tape Silicone Adhesive Single Sided | Discs

Main features

  • 1 mil polyimide film
  • Single side Silicone adhesive
  • >6500V breakdown voltage

Product Description

CAPLINQ LINQTAPE™ PIT1S-ESD Series polyimide tape is a high-temperature resistant, antistatic treated polyimide film mounted with a silicone adhesive. It is designed for both masking and temporary bonding in many high-temperature applications in semiconductor, electronic, automotive, and other general manufacturing industries.

LINQTAPE™ PIT1S-ESD Series polyimide tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 260°C (500°F).


LINQTAPE™ PIT1S-ESD-DCD
 tapes come in varying designs and patterns. This tape can be delivered in a range of die-cut disc sizes with diameters ranging from 1/8" to 12". Custom thicknesses, designs, and diameters are available upon request.

 

Key Features

  • Low peel voltage
  • Anti-static conductive polymer
  • Excellent dielectric properties
Product Family

LINQ PIT1S-ESD-DCD

1. Select Diameter
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Diameter.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Silicone
Adhesive Thickness
38.1 µm
Chemistry Type
Polyimide
Color
Amber
Film Thickness
25.4 µm
Release Liner
None
Single or Double-Sided Adhesive
Single-Sided
Special Layer
Antistatic Polymer Coating
Total Thickness
63.5 μm
Thermal Properties
Temperature Resistance
260 ˚C
Electrical Properties
Breakdown Voltage
>6500 V
Dielectric Strength
256 kV/mm
Volume Resistivity
10000000000000 Ohms⋅cm
Other Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength
19 Oz/in
Elongation
55 %

Additional Information

Product Applications

In sheet form (LINQTAPE PIT1S-ESD Series), the antistatic tapes are used to safely dissipate electrostatic charges before they can build up and cause harmful ESD events to critical electronic components.

These antistatic tapes also have a high dielectric strength which allows them to be used as electrical insulators and isolators. Further to this, these antistatic polyimide tapes have a low peel voltage feature which is important as they generate little voltage when they are unrolled – thereby protecting static-sensitive devices by minimizing the electrostatic charges added when the tape is applied.

This combination of properties makes them suitable for a range of applications including but not limited to batteries, smartphones, tablets, and any other application that requires an anti-static polyimide tape.

In disc form (LINQTAPE PIT1S-ESD-DCD Series), the precut shapes can be peeled right on the release liner and applied. KRAYDEN can also make custom-made stamped polyimide shapes that are stamped according to your specifications. Ask your representative for more information.

The silicone adhesive used makes it better suited to even higher temperature applications, but in the case that a silicone adhesive cannot be used, KRAYDEN offers also a version with an acrylic adhesive, PIT1A-ESD Series.

Application Ideas

  • Protection of static-sensitive devices
  • Temporary bonding of thermocouples for oven profiling
  • Bonding of devices before solder reflow
  • Splicing of Insulation Layers
  • Gold Finger Masking
  • Insulating circuit boards and coils

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers