PIT1A-LO | 1-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1A-LO | 1-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Main features

  • 1 mil polyimide film
  • Non-silicone, low outgassing acrylic adhesive
  • >6000V breakdown voltage

Product Description

LINQTAPE™ PIT1A-LO is an amber high-temperature resistant polyimide film designed for both permanent and temporary bonding in many high-temperature applications. These applications can be found in semiconductor, smartcard, electronic, automotive and aerospace industries. Its low outgassing properties make it a perfect solution for sensitive applications. It has a 1mil backing thickness and 1.5 mil acrylic adhesive. This tape has less than 1% TML and less than 0.1% CVCM values, making it suitable for aerospace applications. 

LINQTAPE™ PIT1A-LO has good adhesion and tensile strength and can operate in temperatures between -29°C to 177°C. It comes in 33 meter (36 yard) rolls of varying widths. LINQTAPE PIT1A polyimide films with acrylic adhesive are available in a range of thicknesses, starting from 0.5 mil (12.7µm) thickness and up. Custom thicknesses are available upon request.

Product Family

LINQ PIT1A-LO

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Adhesive Thickness
50.8 µm
Color
Amber
Film Thickness
25.4 µm
Release Liner
None
Single or Double-Sided Adhesive
Single
Total Thickness
76.2 μm
Thermal Properties
Temperature Resistance
-30 to 175 ˚C
Electrical Properties
Breakdown Voltage
6500 V
Mechanical Properties
Adhesion Strength
50 Oz/in
Elongation
55 %
Tensile Strength (Thin Film)
53 N/cm