PIT1A-FRC | 1-mil Clear Polyimide (Kapton) tape with FR coating

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1A-FRC | 1-mil Clear Polyimide (Kapton) tape with FR coating

Main features

  • 1mil Optically Clear Polyimide
  • Flame retardant acrylic adhesive
  • 4000 V Breakdown Voltage

Product Description

LINQTAPE™ PIT1A-FRC is a clear high-temperature resistant polyimide film designed for both permanent and temporary bonding in many high temperature applications. It’s high breakdown voltage (4,000V) and high temperature resistance make it ideal for applications that require the balancing of multiple properties over a wide temperature range. The FR series has a special flame-retardant acrylic adhesive, which is rated for applications anywhere from –29 °C to 177 °C. Some applications include gold fingers for protection in wave soldering, ground barrier and phase insulation, and outer wrapping for small bobbin wound coils.

LINQTAPE™ PIT1A-FRC film comes in 33 meter (36 yard) rolls of varying widths. LINQTAPE PIT-A polyimide films with acrylic adhesive are available in a range of thicknesses, starting from 0.5 mil (12.7  µm) thickness and up. Custom thicknesses are available upon request.

 

Product Family

LINQ PIT1A-FRC

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Chemistry Type
Polyimide
Color
Clear
Film Thickness
25.4 µm
Special Layer
Flame retardant
Total Thickness
63.5 μm
Electrical Properties
Breakdown Voltage
4000 V
Mechanical Properties
Adhesion Strength
14 Oz/in
Elongation
45 %
Tensile Strength (Thin Film)
35 N/cm