PIT1A-ESD-B | 1 mil Black XC ESD Conductive Polyimide (Kapton) Tape with Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

1 mil Black XC ESD Conductive Polyimide Tape Acrylic Adhesive

Main features

  • 1 mil polyimide film
  • Acrylic adhesive
  • >6500V breakdown voltage

Product Description

LLINQTAPE PIT1A-ESD-Black Series is a high-temperature resistant, antistatic treated polyimide tape with electro-static discharge mounted with an acrylic adhesive. It is designed for both permanent and temporary bonding in many high-temperature applications. This tape has the same mechanical properties as our standard PIT1A-Series products but is black and has a 1µm conductive polymer that provides electro-static discharge and makes the tape anti-static.

LINQTAPE PIT1A-ESD-Black Series tapes get their conductivity by being carbon-loaded. As such the film provides both thermal conductivity as well as antistatic control with a surface resistance of less than 10E9 ohms per square. This product is an alternative to Kapton XC film with an acrylic adhesive layer.

We are moving on to discontinue this SKU and move on to a solution with a release liner. The price is almost the same. This will ensure better protection of the adhesive from pressure and from drying under nonstandard storage conditions. 

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Adhesive Thickness
38.1 µm
Chemistry Type
Polyimide
Color
Black
Film Thickness
25.4 µm
Release Liner
None
Single or Double-Sided Adhesive
Single-Sided
Special Layer
Antistatic Polymer Coating
Thermal Properties
Temperature Resistance
155 ˚C
Electrical Properties
Breakdown Voltage
6500 V
Dielectric Strength
256 kV/mm
Other Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength
25 Oz/in
Elongation
55 %
Tensile Strength (Thin Film)
53.391 N/cm