PIT0.5S | 0.5-mil Polyimide (Kapton) Tape with Silicone Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT0.5S | 0.5-mil Polyimide (Kapton) Tape with Silicone Adhesive

Main features

  • 0.5 mil polyimide film
  • Silicone adhesive
  • >3000 V breakdown voltage

Product Description

LINQTAPE™ PIT0.5S-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. These applications can be found in semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE™ PIT0.5S-Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260°C (500°F

LINQTAPE™ PIT0.5S-Series comes in 33 meter (36 yard) rolls of varying widths. LINQTAPE PIT-S polyimide films with silicone adhesive are available in a range of thicknesses, starting from 0,5 mil (12.7µm) thickness and up. Custom thicknesses are available upon request.

Product Family

LINQ PIT0.5S

1. Select Width
2. Select Length
Price starting from $6.00
Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature Resistance
260 ˚C
Other Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion Strength
12 Oz/in
Elongation
25 %
Tensile Strength (Thin Film)
10 N/cm
General Properties
Adhesive Layer
Silicone
Adhesive Thickness
25.4 µm
Chemistry Type
Polyimide
Color
Amber
Film Thickness
12.7 µm
Release Liner
None
Single or Double-Sided Adhesive
Single-Sided
Special Layer
None
Total Thickness
38.1 μm
Electrical Properties
Breakdown Voltage
>3000 V
Volume Resistivity
10000000000000 Ohms⋅cm