PIT0.5N | 0.5-mil Polyimide (Kapton) Film

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT0.5N | 0.5-mil Polyimide (Kapton) Film

Main features

  • 0.5 mil polyimide film
  • No adhesive
  • >3000V breakdown voltage

Product Description

LINQTAPE PIT0.5-Series is a high-temperature resistant polyimide film designed for both permanent and temporary bonding in many high-temperature applications. These applications can be found in semiconductor, smartcard,
electronic, automotive, and general manufacturing industries. It is ideal for applications that require the balancing of multiple properties over a wide temperature range. LINQTAPE PIT0.5-Series film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 400°C.

LINQTAPE™ PIT0.5N Film comes in 33-meter (36-yard) rolls of varying widths. LINQTAPE PIT-N polyimide films without adhesive are available in a range of thicknesses, starting from 0.5 mil (12.7µm) thickness and up. Custom thicknesses are available upon request.

Key Features:

  • High-temperature applications
  • Thin film without adhesive
  • Excellent electrical properties
Product Family

LINQ PIT0.5N

1. Select Width
2. Select Length
Price starting from $4.33
Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
None
Chemistry Type
Polyimide
Color
Amber
Film Thickness
12.7 µm
Special Layer
None
Total Thickness
12.7 μm
Thermal Properties
Temperature Resistance
400 ˚C
Electrical Properties
Breakdown Voltage
>3000 V
Other Properties
RoHS Compliant
Yes
VOC-Free (100% solids content)
Yes
Mechanical Properties
Elongation
>35 %
Tensile Strength (Thin Film)
20,000 N/cm