OLS-1000HF | Liquid Encapsulant - Two part Epoxy

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OLS-1000HF | Liquid Encapsulant - Two part Epoxy

Main features

  • Liquid epoxy encapsulant
  • LED applications
  • Low Halogen

Product Description

OPTOLINQ OLS-1000HF is a two-part (Part A & Part B), optically clear epoxy casting compound designed for the encapsulation of LED lamps and displays. It features excellent UV resistance, high optical transmittance, good adhesion to a range of substrates, and good thermal shock resistance. It is geared specifically for applications that will not be exposed to temperatures above 125 °C, and where the cost of the encapsulation material is a large percentage of the final part cost. The OLS-1000HF is the Low Halogen version of OLS-1000.

OPTOLINQ OLS-1000HF has been used extensively for low-power LED encapsulation, automatic LED casting, and potting of large optoelectronic modules. Each of these applications relies on the high clarity and other optical properties of the OLS-1000HF as well as its excellent mechanical properties. The OLS-1000 can be colored and diffused by the addition of specific dye concentrates and diffusant concentrates. This product is not made for SMD encapsulation but mainly for DIP packages.

 

 
Product Family

LINQ OLS-1000HF

1. Select Package Type
2. Select Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type and Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
4 hours
Refractive index
1.51
Thermal Properties
Glass Transition Temperature (Tg)
159 °C
Electrical Properties
Dielectric Strength
20 kV/mm
Visible Light Transmission
98 %
Volume Resistivity
6400000000000000 Ohms⋅cm
Chemical Properties
Water Absorption
0.3 %

Additional Information

Processing Instructions

Pre-heat agent A at 45–60 °C for a maximum of 4 h, depending on the temperature and season.

Mix components A and B in a certain proportion and stir uniformly.

Defoam the mixture.

Curing conditions :

  • Size Φ3:            First cure at 130–135 °C/1 h, followed by post cure at 130–135 °C/6–8 h.
  • Size Φ5:            First cure at 125–130 °C/1 h, followed by post cure at 130–135 °C/6–8 h.
  • Sizes Φ8, Φ10: First cure at 105–120 °C/1 h, followed by post cure at 130–135 °C/6–8 h.

 

 Degree of Cure after First Curing
TMA Chart
DSC Curve (Partially Cured and Liquid OLS-1000HF)

 

OLS-1000HF Transmittance Curve
DSC Curve of Fully Cured OLS-1000HF

Using Additives

Optolinq OLS-1000HF can be mixed with diffusing agents or color pastes to achieve customer-specific purposes.

Recommended quantity (in weight %) of various diffusing agents and color pastes to be used with OLS-1000HF:

  • OCP01-R Red Color Paste: 2-5% by weight
  • OCP01-B Blue Color Paste: 1-3% by weight
  • OCP01-G Green Color Paste: 2-4% by weight
  • ODF-10 Diffusing Agent: 2-5% by weight

Values with our latest pastes and agents TBD.

Storage and Handling

OPTOLINQ OLS-1000HF is supplied in cans and jars and should be kept in a cool (10°C – 25°C) dry place (40% – 75% humidity) away from direct sunlight or temperature extremes. Part B is particularly sensitive to moisture, so be sure to remove moisture after using and to keep the lid of the container tightly sealed after use.

Under these conditions, the shelf life of Part A is 6 months and the shelf life of Part B is 3 months. The data contained herein may be reported as typical value and/or range values based on actual test data and are verified on a periodic basis.

 

OLS-1000HF Beta Site Performance in E*

Material Properties

Material

Tg

delta CTE

Curing temperature

Refractive Index

Halogen Content

Resistivity

Hardness

Modulus

Water absorption

Viscosity

KRAYDEN OLS-1000

125

59

110

1.51

Fl, Br, I = < 50 ppm

Cl ~696 ppm

Electrically non-conducting

> 88

3.4 GPa

< 0.35

~1,000

Initial Assessment

Test

Remarks

Shore D

PASSED – Shore D measurements were consistent w/ expected values in TDS

Transmission Test

PASSED – High transmittance at ~905 nm and comparable w/ current material

Degree of cure

PASSED - >90% degree of cure obtained from DSC (also consistent w/ Shore D readings)

Tg

PASSED – Tg values obtained from DSC were close (+/- 20C) from the declared Tg in TDS

Ease of Dispensing

PASSED – Can be dispensed using current tapered plastic dispense needle and current dispensing machine

Curing Profile

PASSED – Compatible w/ current conventional convection oven in the production line

Material Preparation

PASSED – No problems encountered in 1:1 mixing and Thinky Mixer procedure to mix

Sample build using dummy units

  • No other visual defects observed post-cure.
  • No cracks, no delamination (time zero), no voids and bubbles, no leak, no cloudy encapsulation.

Good units build for WHTOL

  • No issues encountered during production build for WHTOL.

 

 