OCA | optically clear adhesive film

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

OCA | optically clear adhesive film

Main features

  • 91% Light transmittance
  • 1 Optical haze
  • Acid free

Product Description

LINQTAPE OCA is a film made out of Optically Clear Adhesive (OCA) backed on a PET substrate. OCA is a double-sided adhesive tape that is matrix-free, meaning it contains no supporting material.

LINQTAPE OCA has exceptional high visible light transmittance and low resistivity, making OCA film one of the most versatile and high-performance conductive materials available.

 

Applications include:

  • Transparent device bonding: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
  • Display assembly: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
  • Areospace and militairy optic assembly: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
  • Lenses: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.

 

Product Family

LINQ OCA

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Adhesive Thickness
10 µm
Release Liner
Yes
Total Thickness
60 μm
Thermal Properties
Operating Temperature
-40 ~ 110 °C
Electrical Properties
Visible Light Transmission
>92 %
Other Properties
RoHS Compliant
Yes
Mechanical Properties
Adhesion Strength
70 Oz/in

Additional Information

Key Optical and Physical Properties:

  • Optical Haze: <1

  • Light Transmittance: >91%

  • Physical Glue: >1500 g/25mm

  • Release Force of Light Release Film: <10 g/25mm

  • Release Force of Heavy Release Film: 25-30 g/25mm

Environmental Test Results:

  • Hot and Humid (60°C, 90%RH, 240 Hours): PASS
  • Thermal Shock (40°C~80°C, 30min/cycle, 200 Cycles): PASS
  • High Temperature (80°C, 240 Hours): PASS
  • Low Temperature (-40°C, 240 Hours): PASS

Key Features:

  1. Excellent optical performance: achieving transmittance of 92% or higher, with haze below 1.
  2. Acid-free: material with no corrosion impact on the adherend.
  3. Durability: Demonstrates durability without yellowing or bubble formation.
  4. Performance in variable conditions: Exhibits excellent performance under high and low-temperature conditions.
  5. Price die cutting: Ensures precise die-cutting with no overflow.

Leading Brands Trust in Our Products and Services