ITO-125 | 125 μm Indium Tin Oxide film

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

ITO-125 | 125 μm Inidium Tin Oxide film

Main features

  • 85% Light transmittance
  • 125um thickness
  • Ease of processing

Product Description

LINQTAPE ITO-125 is a transparent 125μm film made out of Indium Tin Oxide (ITO) backed on a PET substrate. ITO-125 is a n-type semiconductor material, which offers a unique combination of properties that are useful for a wide range of applications.

LINQTAPE ITO-125 has exceptional high visible light transmittance and low resistivity, making ITO conductive film one of the most versatile and high-performance conductive materials available. It empowers innovation across industries, and serves as a vital component in touchscreen displays, solar panels, and other cutting-edge technologies.

Applications:

  • Flat panel display devices: With exceptional light transmittance of up to 85%, our ITO Conductive Film guarantees crystal-clear visibility within the visible spectral region.
  • Solar cells: The layers ensure long-lasting performance even in challenging environments and boast superior ultraviolet (UV) absorption, with an absorption rate exceeding 85%, this film offers excellent UV protection.
Product Family

LINQ ITO-125

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Electrical Properties
Surface Resistivity
5±2 Ohms/sq
Visible Light Transmission
>85 %

Additional Information

Indium Tin Oxide films Feature:

  • Outstanding Electrical Conductivity: Achieving impressively low resistivity of up to 10^-4Ω∙cm, this film ensures efficient electrical conductivity for various applications.
  • High Visible Light Transmittance: With exceptional light transmittance of up to 85%, our ITO Conductive Film guarantees crystal-clear visibility within the visible spectral region.
  • UV Absorption: Boasting superior ultraviolet (UV) absorption, with an absorption rate exceeding 85%, this film offers excellent UV protection.
  • Infrared Reflectivity: With an infrared (IR) reflectivity exceeding 80%, it efficiently manages heat and radiation, making it suitable for diverse applications.
  • Microwave Attenuation: Our ITO Conductive Film excels in microwave attenuation, with an attenuation rate of up to 85%, making it an ideal choice for applications requiring interference reduction.
  • Exceptional Durability: The thin layer exhibits high hardness, wear resistance, and chemical corrosion resistance, ensuring long-lasting performance even in challenging environments.
  • Ease of Processing: This film offers excellent machining performance and is easy to etch, allowing for effortless customization to meet your specific requirements.