DCT-PVC80NUV | Polymerized Vinyl Chloride Dicing Tape

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

DCT-PVC80NUV | Polymerized Vinyl Chloride Dicing Tape

Main features

  • 80 µm film thickness
  • Translucent Film
  • Acrylic non UV adhesive

Product Description

LINQTAPE™ DCT-PVC80NUV is a polymerized vinyl chloride tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Its strong adhesion ensures the wafer remains secure during different manufacturing processes like die-cutting.  The security the tape provides prevents wafer damage, whiskers, soaking and allows for cleaner cuts. 

LINQTAPE™ DCT-PVC80NUV is a translucent 80µm film, with a one-sided 10µm acrylic adhesive layer, and backed with a PET liner. It is ideal for small chips. This product can be customized according to the customer's needs.  

Key Features

  • Strong adhesion to prevent wafer damage
  • Can be used with uneven surfaces
  • Antistatic
  • High Transparency
  • High and evenly distributed elasticity 
  • High heat tolerance (60 °C for a few minutes)

 

Application Ideas

  • Die -cutting
  • Great for small silicon wafers
Product Family

LINQ DCT-PVC80NUV

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Adhesive Thickness
10 µm
Appearance
Translucent
Film Thickness
70 µm
Total Thickness
80 μm
Mechanical Properties
Adhesion Strength
5760 Oz/in
Elongation
271 lengthwise, 324 crosswise %
Tensile Strength (Thin Film)
27 lengthwise, 20 crosswise N/cm