BMC-7600H-BDF  | Black Optical Molding Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

TC-7600H-BDF | Black Optical Molding Compound

Main features

  • High performance
  • Fine pitch RGB
  • Black with wet method

Product Description

OPTOLINQ BMC-7600H-BDF is a high-performance, black coloured, optically clear epoxy developed for small space RGB applications. This single component epoxy exhibits excellent adhesion and stability at high temperature that helps achieve great package performance and long life. It works very similar, if not better than XX600H product types.

BMC-7600H-BDF gets its black colour not by powder mixing but with a wet method . This low stress, led encapsulation epoxy passes TCT, PCT and moisture reliability testing on EMC1010 package standard. It is a reliable product that passes reflow thermal cycling test at 85°C @85% relative humidity and is ideal for fine pitch RGB.

Product Family

LINQ BMC-7600H-BDF

1. Select Package Type
2. Select Pellet Size
3. Select Pellet Weight
4. Select Transmittance
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Package Type, Pellet Size, Pellet Weight and Transmittance.

Technical Specifications

General Properties
Refractive index
1.56
Specific Gravity
1.67
Thermal Properties
Glass Transition Temperature (Tg)
135 °C
Chemical Properties
Water Absorption
0.11 %
Physical Properties
Spiral Flow @ 175°C
150 - 250 cm
Curing Conditions
Transfer Pressure
10 - 40 kg/cm2
Transfer Time
20 - 50 s

Additional Information

The epoxy molding compound is sealed with aluminum laminated bags, in quantities of 1kg/bag in a 10kg/box.
Each carton box legibly provides the following information: Item name, Size, Lot NO, Quantity, MFG date, EXP date, and other information customer required.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers