BCP-3502 | 130℃ RTI Busbar Coating Powder

Harmonization Code : 3907.30.20 | Epoxide resins of a kind used for coating in powder form

BCP-3502 | Medium Voltage Busbar Coating Powder

Main features

  • Black, red halogen-free epoxy coating powder
  • Flexible use for low and medium voltage systems
  • High heat resistance (RTI 130 °C) with UL94 V-0 rating

Product Description

LINQSOL BCP-3502 is a halogen-free epoxy powder coating engineered for superior electrical insulation in busbar systems. It offers rapid build-up and excellent coating uniformity across a broad thickness range, from 0.1 mm to 2.0 mm, making it a versatile solution for various electrical insulation needs. LINQSOL BCP-3502 is available in different colors. Contact us for more information. 

Product Key Features

  • High Thermal Endurance — Meets UL 746B Relative Thermal Index (RTI) of 130 °C for reliable performance at elevated temperatures.
  • Superior Dielectric Strength — Provides exceptional electrical insulation properties.
  • Flame Retardant — Achieves a UL94 V0 rating for enhanced safety.
  • Can be applied using electrostatic spray or fluidized bed methods.

Product Key Applications

  • Low-voltage busbar systems up to 600 V.
  • Medium-voltage busbar applications up to 38 kV.

 

Product Family

LINQ BCP-3502

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Particle size (D50)
45-60 um
Thermal Properties
UL 94 Rating
V-0
Electrical Properties
Dielectric Strength
45 kV/mm
Chemical Properties
Water Absorption
0.3 %

Additional Information

LINQSOL BCP-3502 Recommended Curing Conditions

Parameter Value Unit
Preheat Temperature 150-180℃ ℃
Preheat Duration 5-12 s
Curing Temperature 180 ℃
Curing Duration at 180℃ 45-55 min

 