BCP-1504 | Low voltage Busbar Coating Powder

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

BCP-1504 |  Low voltage Busbar Coating Powder

Main features

  • Blue Color
  • Quick thickness build
  • RTI Class B

Product Description

LINQSOL BCP-1504 is a blue or red, busbar epoxy coating powder. It applies at low voltage  copper and alumina busbars (600V) with a coating thickness of 0.3~1mm. With its low pick up  temperature, BCP-1504 builds up quickly at small busbars and performs excellent coating results. It brings high productivity with low pre-heat temperature and quick curing. Due to its fine-grind process, it can be used with both electrostatic spray and fluidized bed dipping. 

Key Features:

  • Comparable with DK15-0463
  • Good adhesion to copper, alumina 
  • Low pick up temperature 
  • High powder build rate 
  • Both electrostatic spray and fluidized bed coating

Recommended coating Temperature:

  • 150 – 180 °C. (200 °C x 15 min)
Product Family

LINQ BCP-1504

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue and customized
Process Method
Fluidized bed, electrostatic spray
Specific Gravity
1.52
Thermal Properties
Glass Transition Temperature (Tg)
100 °C
UL 94 Rating
V-0
Electrical Properties
Breakdown Voltage
35 V
Volume Resistivity
0.000000000000001 Ohms⋅cm
Other Properties
RoHS Compliant
YES
Mechanical Properties
Edge Coverage
45 %
Impact Strength
500 mm

Additional Information

 

BCP-1504 Fluidized Bed Coating Performance 
Preheat Temperature Dip Times Minimum Coat Thickness Breakdown Voltage Pass
200°C 1 0.43 mm >20 kV
240°C 1 0.43 mm >20 kV
240°C 2 0.48 mm >20 kV
240°C 3 0.70 mm  >20 kV
240°C 4 0.85 mm  >20 kV
240°C 8 1.30 mm  >20 kV

Busbar for testing: Aluminum strip (75mm x 50mm x 5mm)

Breakdown volatge test: DC holiday detector

OBSERVATION

  • Coating appearance: Smooth, no-dripping, great edge coverage
  • Coating process: Quick build rate on thickness, low pick up temperature;
  • Preheat temperature: 240°C preheat temperature with 1 dip reaches 0.5mm, which is thicker than 1 dip @200°C, but appears small-size sag. With multiple dips, the surface becomes smooth again.

DISCUSSION

BCP-1504 presents good coating results with preheat temperature 200°C.  BCP-1504 has low pickup temperature and it is designed to coat on small size busbar with quick build rate.

 

BCP-1504 Powders In Fluidized Bed

Storage

Store in a ventilated, dry, and clean environment below 25°C. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, the product has a shelf life of 6 months.

Precautions

  • Avoid long-term skin contact. Powder that touched the skin should be rinsed off quickly.

  • During operation dust-proof masks should be used to avoid inhalation.

  • Keep the oven temperature stable, so as not to affect the colour and quality of the coating due to excessive temperature deviation.

  • The concentration of dust should be controlled within a safe range to avoid malfunction of the coating equipment.

Linqsol Busbar Coating Products Selection Guide

 

BCP-1000

BCP-1504

BCP-1507

BCP-1509

Specific Gravity, g/cc

1.45±0.05

1.52±0.05

1.50

1.50

Glass Plate Flow

18-22mm@150°C, 45°

10-22mm@150°C, 60°

19-20 mm@180°C

19-20 mm@180°C

Hot Plate Gel Time

70 sec@150°C

45±15 sec@160°C

60 sec@180°C

60 sec@180°C

Edge Coverage, %

45

45

45

45

Hardness, shore D

>80

>90

-

-

Impact Resistance, cm

>50

>50

>50

>50

Dielectric Strength (kV/mm)

>42

>35

>35

>35

Flammability, UL94

V-0

V-0

V-0

V-0

Min. Coating Thickness

0.3mm

0.3mm

0.1mm

0.3mm

Max. Coating Thickness

1mm

1mm

2mm

3mm

Electrostatic Spray

■■■

■■□

■■■

■■■

Dip Coating

■□□

■■■

■■■

■■■

Available Color

●●●●●

●●

●●●●●

●

Preheat Temperature

180~240 °C

150~180 °C

180~230 °C

180~230 °C

Curing Conditions

200°C x 15min

200°C x 15min

200°C x 30min

200°C x 30min

 